A correction fluid and a new type of technology, applied in the field of correction fluid, can solve problems such as uneven application, poor application effect, and difficult adhesion of the covering layer, and achieve the effects of uniform application, good rewriting performance, and good application effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0009] A new type of correction fluid, comprising 25% of deionized water, 10% of water-based acrylic resin, 40% of titanium dioxide, 10% of organic silicon, and 15% of acrylate emulsion, the above ingredients are calculated by weight percentage.
[0010] The preparation method is: add 25% deionized water into a four-neck bottle, add 10% water-based acrylic resin, heat to raise the temperature to 85°C, and after all of it is dissolved, lower the temperature to room temperature, and then add 40% titanium dioxide and 10% silicone, stir until evenly mixed, take out the mixture, grind it with a grinder to a fineness of 15-60μm, then put the ground mixture into a beaker, add 15% acrylate emulsion, stir until mixed Evenly, this correction fluid is obtained.
Embodiment 2
[0012] A new type of correction fluid comprises 15% of deionized water, 15% of water-based acrylic resin, 50% of titanium dioxide, 5% of organic silicon, and 15% of acrylic emulsion. The above components are calculated by weight percentage.
[0013] The preparation method is: add 15% deionized water into a four-neck bottle, add 15% water-based acrylic resin, heat to raise the temperature to 85°C, and after it is completely dissolved, lower the temperature to room temperature, and then add 50% titanium dioxide and 5% silicone, stir until evenly mixed, take out the mixture, grind it with a grinder to a fineness of 15-60μm, then put the ground mixture into a beaker, add 15% acrylate emulsion, stir until mixed Evenly, this correction fluid is obtained.
Embodiment 3
[0015] A new type of correction fluid, comprising 32% of deionized water, 5% of water-based acrylic resin, 30% of titanium dioxide, 3% of organic silicon, and 30% of acrylic emulsion, the above ingredients are calculated by weight percentage.
[0016] The preparation method is: add 32% deionized water into a four-neck bottle, add 5% water-based acrylic resin, heat to raise the temperature to 85°C, and after it is completely dissolved, lower the temperature to room temperature, and then add 30% titanium dioxide and 3% silicone, stir until evenly mixed, take out the mixture, grind it with a grinder to a fineness of 15-60μm, then put the ground mixture into a beaker, add 30% acrylate emulsion, stir until mixed Evenly, this correction fluid is obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com