Warp-knitted insulation fabric and production method and application thereof
A kind of fabric and warp knitting technology, which is applied in warp knitting, application, textiles and papermaking, etc. It can solve the problems of rough hand feeling, easy detachment, low yarn strength, etc., and achieve the effect of excellent air permeability and heat preservation, and comfortable hand feeling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0038] The face comb adopts 30D-24f-polyester FDY, and the bottom comb adopts 150D-42f-viscose FDY. Among them, the strength of viscose FDY is 2.1cN / dtex, and the warping tension of viscose FDY is about 30.5g. The tissue adopts GB1:10 / 12 / / , GB2:12 / 10 / / , on a 28G Tricker warp knitting machine The gray cloth is woven, and then the gray cloth is refined and desized (refining agent 0.5g / l, 90°C), intermediate setting (190°C), one-bath two-step dyeing (disperse dyeing 130°C, reactive dyeing 65°C ), resin finishing (antistatic agent 10g / L, softener 10g / L), finishing and setting (160°C), the obtained polyester yarn content is 16%, viscose yarn content is 84%, and the weight is about 201g / m 2 warp knitted fabric. The specific parameters are shown in Table 1.
Embodiment 2
[0040] The face comb adopts 30D-24f-polyester FDY, and the bottom comb adopts 150D-42f-viscose FDY. Among them, the strength of viscose FDY is 2.1cN / dtex, and the warping tension of viscose FDY is about 30.5g. The tissue adopts GB1:10 / 23 / / , GB2:12 / 10 / / , on a 28G Tricker warp knitting machine The gray cloth is woven, and then the gray cloth is refined and desized (refining agent 0.5g / l, 90°C), intermediate setting (190°C), one-bath two-step dyeing (disperse dyeing 130°C, reactive dyeing 65°C ), resin finishing (antistatic agent 10g / L, softener 10g / L), finishing and setting (160°C), the obtained polyester yarn content is 22%, viscose yarn content is 78%, and the weight is about 217g / m 2 warp knitted fabric. The specific parameters are shown in Table 1.
Embodiment 3
[0042]The face comb adopts 30D-36f-polyester FDY, and the bottom comb adopts 120D-48f-viscose FDY. Among them, the strength of viscose FDY is 1.9cN / dtex, and the warping tension of viscose FDY yarn is about 24.5g. The gray cloth is woven on the knitting machine, and then the gray cloth is refined and desized (refining agent 0.5g / l, 90°C), intermediate setting (190°C), one-bath two-step dyeing (disperse dyeing 130°C, reactive dyeing 65°C), resin finishing (antistatic agent 10g / L, softener 10g / L), finishing and setting (160°C), to obtain a polyester yarn content of 35%, viscose yarn content of 65%, and a weight of about 208g / m 2 warp knitted fabric. The specific parameters are shown in Table 1.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com