A beneficiation process for improving the quality and reducing silicon of iron concentrate
A technology of iron concentrate and process, which is applied in the field of beneficiation process for improving the quality of iron concentrate and reducing silicon, which can solve the problems of failing to meet the requirements of pipeline transportation, resource loss, and high silicon grade, so as to improve production efficiency and reduce environmental pollution , the effect of low requirements
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] The iron grade is 58%, the silicon grade is 10%, and the iron concentrate with a particle size of -200 mesh accounts for 72% is finely ground to the ore powder with a particle size of -325 mesh accounting for 80%. The ore powder after grinding is magnetically separated by a CTB / N / S-1230 magnetic separator with a magnetic induction intensity of 800T to obtain a section of weak magnetic concentrate and a section of weak magnetic tailings. A section of weak magnetic tailings is magnetically separated by a SLon-2000 magnetic separator with a magnetic induction intensity of 12000T to obtain a section of strong magnetic concentrate and a section of strong magnetic tailings. The first stage of weak magnetic concentrate is magnetically separated by CTB / N / S-1230 magnetic separator with a magnetic induction intensity of 1000T to obtain the second stage of weak magnetic concentrate and the second stage of weak magnetic tailings, and the second stage of weak magnetic tailings is ret...
Embodiment 2
[0043] The iron grade is 60%, the silicon grade is 9%, and the iron concentrate with a particle size of -200 mesh accounts for 75% is finely ground to a particle size of -325 mesh and accounts for 80% of the ore powder. The ore powder after grinding is magnetically separated by a CTB / N / S-1024 magnetic separator with a magnetic induction intensity of 1000T to obtain a section of weak magnetic concentrate and a section of weak magnetic tailings. A section of weak magnetic tailings is magnetically separated by a SLon-1500 magnetic separator with a magnetic induction intensity of 14000T to obtain a section of strong magnetic concentrate and a section of strong magnetic tailings. The first stage of weak magnetic concentrate is magnetically separated by a CTB / N / S-1024 magnetic separator with a magnetic induction intensity of 1200T to obtain the second stage of weak magnetic concentrate and the second stage of weak magnetic tailings, and the second stage of weak magnetic tailings is r...
Embodiment 3
[0045] The iron grade is 59%, the silicon grade is 8%, and the iron concentrate with a particle size of -200 mesh accounts for 70% is finely ground to the ore powder with a particle size of -325 mesh accounting for 80%. The ore powder after grinding is magnetically separated by a CTB / N / S-924 magnetic separator with a magnetic induction intensity of 900T to obtain a section of weak magnetic concentrate and a section of weak magnetic tailings. A section of weak magnetic tailings is magnetically separated by a SLon-1000 magnetic separator with a magnetic induction intensity of 10000T to obtain a section of strong magnetic concentrate and a section of strong magnetic tailings. The first stage of weak magnetic concentrate is magnetically separated by a CTB / N / S-924 magnetic separator with a magnetic induction intensity of 800T to obtain the second stage of weak magnetic concentrate and the second stage of weak magnetic tailings, and the second stage of weak magnetic tailings is retur...
PUM
| Property | Measurement | Unit |
|---|---|---|
| magnetic flux density | aaaaa | aaaaa |
| magnetic flux density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 