A fire retardant coating and environmental protection technology, applied in the field of coatings, can solve the problems of poor texture of fire retardant coatings, special working environment, difficult to meet the requirements of fire retardant coatings, etc., to achieve fine coating, environmental protection and human safety, foaming efficiency and uniform effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] An environment-friendly fireproof coating for lost foam is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0015] 30 parts of water-based mixed resin composed of acrylate, flame-retardant amino resin and chloroether resin according to the weight ratio of 1:1:4, 8 parts of acrylic acid, 3 parts of titanium dioxide, 2 parts of tricresyl phosphate, 3 parts of wood fiber, antimony oxide 0.4 parts, 3 parts of chlorinated paraffin wax, 2 parts of slaked lime, 0.5 parts of maleic anhydride, 2 parts of char-forming agent composed of sucrose and pentaerythritol in a weight ratio of 1:2, 15 parts of MADE high boiling point environmental protection solvent.
Embodiment 2
[0017] An environment-friendly fireproof coating for lost foam is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0018] 35 parts of water-based mixed resin composed of acrylate, flame-retardant amino resin and chloroether resin in a weight ratio of 1:1:4, 9 parts of acrylic acid, 4 parts of titanium dioxide, 3 parts of tricresyl phosphate, 4 parts of wood fiber, antimony oxide 0.5 parts, 4 parts of chlorinated paraffin, 3 parts of slaked lime, 0.6 parts of maleic anhydride, 2 parts of char-forming agent composed of sucrose and pentaerythritol in a weight ratio of 1:2, 18 parts of MADE high boiling point environmental protection solvent.
Embodiment 3
[0020] An environment-friendly fireproof coating for lost foam is characterized in that the components of the raw materials are composed as follows in parts by weight:
[0021] 40 parts of water-based mixed resin composed of acrylate, flame-retardant amino resin and chloroether resin according to the weight ratio of 1:1:4, 10 parts of acrylic acid, 5 parts of titanium dioxide, 4 parts of tricresyl phosphate, 5 parts of wood fiber, antimony oxide 0.6 parts, 5 parts of chlorinated paraffin, 4 parts of slaked lime, 0.8 parts of maleic anhydride, 3 parts of char-forming agent composed of sucrose and pentaerythritol in a weight ratio of 1:2, 20 parts of MADE high boiling point environmental protection solvent.