Adhesion agent, preparation method thereof and corrugated board
A corrugated cardboard and adhesive technology, applied in the field of corrugated cardboard, can solve the problems of increasing the cost of corrugated boxes, and achieve the effects of improving compressive strength and breaking strength, reducing contact angle, and improving adhesive strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0054] The embodiment of the present invention also provides a preparation method of the adhesive in any of the above embodiments, which includes a mixing and stirring step: adding the raw materials of the adhesive in any of the above embodiments into a stirring container, mixing and stirring to form the said adhesive. In the preparation method of the embodiment of the present invention, the order and manner of adding each raw material may not be particularly limited, for example, all the raw materials may be added to the stirring vessel at the same time or in an irregular order for stirring.
[0055] In particular, in a preferred embodiment of the present invention, it is preferred to prepare the adhesive in a set order and manner of addition. Figure 4 is a schematic flowchart of a method for preparing an adhesive according to an embodiment of the present invention. see Figure 4 The mixing and stirring step in the method for preparing the adhesive according to the embodim...
Embodiment 1
[0065] Take the raw materials by the following weight: 1000kg of water, 283kg of cornstarch, 35.8kg of aqueous sodium hydroxide solution (equivalent to 9kg of sodium hydroxide) with a concentration of 25%, 4kg of moisture-resistant agent red glue, 2kg of moisture-resistant agent white glue, and bridging agent 12.5kg, borax 2.5kg.
[0066] a. Add 1000kg of water to the stirring vessel and heat it to about 25°C;
[0067] B, add 18.8kg sodium hydroxide aqueous solution in stirring vessel while stirring, then add 283kg cornstarch in stirring vessel, stir about 2 minutes;
[0068] c. Add 4kg of anti-humidity agent red glue, remaining 17kg of sodium hydroxide aqueous solution, and 2.4kg of anti-humidity agent white glue into the stirring container, and stir until the viscosity of the fluid in the stirring container reaches about 20 seconds;
[0069] d. Add 12.5kg bridging agent to the stirring container, and stir until the viscosity of the fluid in the stirring container reaches ab...
Embodiment 2
[0072] Take the raw materials by the following weight: 1000kg of water, 220kg of cornstarch, 30kg of aqueous sodium hydroxide solution (equivalent to 6kg of sodium hydroxide) with a concentration of 20%, 1kg of anti-humidity agent red glue, 1kg of anti-humidity agent white glue, and 7kg of bridging agent , borax 1kg.
[0073] a. Add 1000kg of water to the stirring container and heat it to about 20°C;
[0074] B, add 9kg sodium hydroxide aqueous solution in stirring container while stirring, then add 220kg cornstarch in stirring container, stir about 5 minutes;
[0075] c. Add 1kg of moisture resistant red glue, 21kg of sodium hydroxide aqueous solution, and 1kg of moisture resistant white glue into the stirring container, and stir until the viscosity of the fluid in the stirring container reaches about 10 seconds;
[0076] d. Add 7kg bridging agent to the stirring container, and stir until the viscosity of the fluid in the stirring container reaches about 30 seconds;
[0077...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com