A fire-proof and heat-retaining real stone paint and preparation method thereof
A technology for fire-proof thermal insulation and real stone paint, which is applied in the field of coatings, can solve the problems of poor coordination between ordinary real stone paint and thermal insulation walls, easy cracks, etc., and achieves the effects of good thermal insulation, good waterproof ability and strong decoration.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] The fireproof and heat preservation real stone paint is prepared according to the following steps:
[0031] (1) Prepare prefabricated solution:
[0032] Add 307 parts of water into the container, then add 1.5 parts of hydroxyethyl cellulose, and disperse for 30 minutes at a speed of 1200 rpm, so that the mixture is uniformly mixed without particles; then add 1 part of AMP-95 multifunctional additive, and 1200 rpm Disperse for 20 minutes at a speed of 1 / min;
[0033] Then add 180 parts of foaming catalyst ammonium polyphosphate, 40 parts of foaming agent melamine, 35 parts of carbon forming agent pentaerythritol, 365 parts of silicon acrylic emulsion, 20 parts of film-forming aid alcohol ester; Stir for 10 minutes;
[0034] Then add 1 part of BIT fungicide and 1 part of water, after mixing, add 3 parts of BIT fungicide and 2 parts of water, and stir at 500 rpm for 20 minutes.
[0035] (2) Put 255 parts of the prefabricated solution obtained in step (1) into the mixer,...
Embodiment 2
[0037] The fireproof and heat preservation real stone paint is prepared according to the following steps:
[0038] (1) Prepare prefabricated solution:
[0039] Add 312 parts of water into the container, then add 3 parts of hydroxyethyl cellulose, and disperse for 20 minutes at a speed of 1500 rpm, so that the mixture is uniformly mixed without particles; then add 2 parts of AMP-95 multifunctional additive, and 1500 rpm Disperse for 20 minutes at a speed of 1 / min;
[0040] Then add respectively 200 parts of foaming catalyst ammonium polyphosphate, 55 parts of foaming agent melamine, 60 parts of carbon forming agent pentaerythritol, 785 parts of silicon-acrylic emulsion, 27 parts of film-forming aid alcohol ester; Stir for 5 minutes;
[0041] Then add 2 parts of BIT bactericide and 3 parts of water, after mixing, add 3.5 parts of BIT bactericide and 5 parts of water, and stir at 800 rpm for 10 minutes.
[0042] (2) Put 270 parts of the prefabricated solution obtained in step ...
Embodiment 3
[0044] The fireproof and heat preservation real stone paint is prepared according to the following steps:
[0045] (1) Prepare prefabricated solution:
[0046] Add 310 parts of water into the container, then add 2 parts of hydroxyethyl cellulose, and disperse for 25 minutes at a speed of 1400 rpm, so that the mixture is uniformly mixed without particles; then add 1.5 parts of AMP-95 multifunctional additive, and 1300 rpm Disperse for 15 minutes at a speed of 1 / min;
[0047] Then add respectively 190 parts of foaming catalyst ammonium polyphosphate, 50 parts of foaming agent melamine, 45 parts of carbon forming agent pentaerythritol, 500 parts of silicon-acrylic emulsion, 25 parts of film-forming aid alcohol ester; Stir for 8 minutes;
[0048] Then add 1.5 parts of BIT fungicide and 2 parts of water, after mixing, add 3 parts of BIT fungicide and 3 parts of water, and stir for 15 minutes at a speed of 600 rpm.