Normal temperature asphalt modifier, normal temperature modified asphalt and warm mix cold asphalt concrete
A technology of normal-temperature asphalt and modified asphalt, which is applied in the field of normal-temperature asphalt modifier, normal-temperature modified asphalt and warm-mixed cold-paved asphalt concrete. Long service life, good adaptability, and the effect of delaying the aging of asphalt
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] The normal temperature asphalt modifier is a mixture of waste engine oil, rubber tire powder and plastic extract; the mass ratio of waste engine oil, rubber tire and plastic extract is 1:2:6.
[0037] Specifically, the plastic extract is a mixture of aromatic hydrocarbons obtained by pyrolysis at 600-900°C, light gasoline and tar, wax obtained by pyrolysis at 400-500°C, and chains obtained by catalytic cracking at 400-600°C. A mixture of alkanes and alkenes. Specifically, the mixing mass ratio of the three is 1:2:1 in turn.
[0038] The particle size of the rubber tire powder used is 10-80 μm.
Embodiment 2
[0040] The normal temperature asphalt modifier is a mixture including waste engine oil, rubber tire powder and plastic extract; wherein the mass ratio of waste engine oil, rubber tire and plastic extract is 1:1:4.
[0041] Specifically, the plastic extract is a mixture of aromatic hydrocarbons obtained by pyrolysis at 600-900°C, light gasoline and tar, wax obtained by pyrolysis at 400-500°C, and chains obtained by catalytic cracking at 400-600°C. A mixture of alkanes and alkenes. Specifically, the mixing mass ratio of the three is 1:2:1 in turn.
[0042] The particle size of the rubber tire powder used is 10-80 μm.
Embodiment 3
[0044] The normal temperature asphalt modifier is a mixture including waste engine oil, rubber tire powder and plastic extract; the mass ratio of waste engine oil, rubber tire and plastic extract is 1:3:8.
[0045] Specifically, the plastic extract is a mixture of aromatic hydrocarbons obtained by pyrolysis at 600-900°C, light gasoline and tar, wax obtained by pyrolysis at 400-500°C, and chains obtained by catalytic cracking at 400-600°C. A mixture of alkanes and alkenes. Specifically, the mixing mass ratio of the three is 1:2:1 in turn.
[0046] The particle size of the rubber tire powder used is 10-80 μm.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com