Rapid Diagnostic Test Strips
A technology for rapid diagnosis and test strips, applied in measuring devices, instruments, fluorescence/phosphorescence, etc., can solve the problem that colloidal gold immunochromatography test strips cannot meet clinical testing, colloidal gold test strips have low sensitivity and cannot reach Requirements and other issues to achieve high social and economic value, high sensitivity, and strong specificity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0052] Embodiment 1, a kind of rapid diagnosis test strip based on homogeneous chemiluminescence technology, comprises PVC bottom plate 1, sample pad 2, glass fiber pad 3, is coated with C line (that is, control line) 6 and T line (that is, Nitrocellulose membrane 4, absorbent pad 5 of test line) 7.
[0053] A nitrocellulose membrane 4 is fixedly arranged on the upper surface of the PVC base plate 1, and a glass fiber pad 3 and a water-absorbing pad 5 are respectively arranged on both sides of the nitrocellulose membrane 4; Except that the upper surface of the left end of 4 is fixedly connected, the remaining lower surface of the glass fiber pad 3 is fixedly connected with the upper surface of the PVC bottom plate 1; except that the lower surface of the left end of the absorbent pad 5 is fixedly connected with the upper surface of the right end of the nitrocellulose membrane 4 , the remaining lower surface of the absorbent pad 5 is fixedly connected to the upper surface of the...
Embodiment 2
[0074] Embodiment 2, a kind of rapid diagnosis test strip based on homogeneous chemiluminescent technology, comprises PVC bottom plate 1, sample pad 2, glass fiber pad 3, is coated with C line (that is, control line) 6 and T line (that is, Nitrocellulose membrane 4, absorbent pad 5 of test line) 7.
[0075] A nitrocellulose membrane 4 is fixedly arranged on the upper surface of the PVC base plate 1, and a glass fiber pad 3 and a water-absorbing pad 5 are respectively arranged on both sides of the nitrocellulose membrane 4; Except that the upper surface of the left end of 4 is fixedly connected, the remaining lower surface of the glass fiber pad 3 is fixedly connected with the upper surface of the PVC bottom plate 1; except that the lower surface of the left end of the absorbent pad 5 is fixedly connected with the upper surface of the right end of the nitrocellulose membrane 4 , the remaining lower surface of the absorbent pad 5 is fixedly connected to the upper surface of the ...
PUM
| Property | Measurement | Unit |
|---|---|---|
| diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com