Preparing method for disproportionated rosin potash soap with solid content of 80%
A technology for disproportionating rosin potassium soap and disproportionating rosin is applied in the directions of chemical instruments and methods, preparations for skin care, cosmetics, etc. Improve success rate, good quality effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Add 95 parts of solid disproportionated rosin and 55 parts of 25% potassium hydroxide solution into the saponification reaction kettle, heat to 80°C while stirring evenly, first carry out saponification reaction for 1 hour, then add 0.2 parts of hydrogen peroxide, and stir for 0.5 hours , and then cooled and discharged to obtain disproportionated rosin potassium soap with a solid content of 80%.
Embodiment 2
[0021] Add 100 parts of solid disproportionated rosin and 65 parts of 22.5% potassium hydroxide solution into the saponification reaction kettle, heat to 90°C while stirring evenly, first carry out saponification reaction for 1.5 hours, then add 0.2 parts of hydrogen peroxide, and stir for 0.5 hours , and then cooled and discharged to obtain disproportionated rosin potassium soap with a solid content of 80%.
Embodiment 3
[0023] Add 105 parts of solid disproportionated rosin and 80 parts of 20% potassium hydroxide solution into the saponification reaction kettle, heat it to 100°C while stirring evenly, first carry out saponification reaction for 2 hours, then add 0.2 parts of hydrogen peroxide, and stir for 0.5 hours , and then cooled and discharged to obtain disproportionated rosin potassium soap with a solid content of 80%.
[0024] Solid content 80% disproportionated rosin potassium soap technical index table 1 of the present invention:
[0025] Table 1
[0026] .
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More