A catalyst and titanium dioxide technology, applied in the field of preparation of high-efficiency new sulfur-fixing catalysts, can solve the problems of ecological environment damage, atmospheric environmental pollution, etc., and achieve the effects of reducing the amount of coal burning, burning fully, and reducing emissions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A method for preparing sulfur fixation catalyst, the specific raw materials and methods are as follows:
[0020] (1) Weigh parts by weight Weigh the following raw materials: 280 parts of water, 250 parts of glycerol, 60 parts of sodium carbonate, 110 parts of sodium methacrylate sulfonate, 130 parts of sodium gluconate, 120 parts of titanium dioxide, and 50 parts of triethanolamine. Titanium dioxide is a nanometer titanium dioxide material obtained after modification treatment.
[0021] (2) Add sodium carbonate, sodium methacrylate sulfonate, and sodium gluconate to 3 / 4 of the water, and stir thoroughly for 1 hour with a stirring tank to prepare mixed solution A;
[0022] (3) Add titanium dioxide to the remaining 1 / 4 of the water and stir with a stirring tank for 30 minutes, then add glycerol and triethanolamine and stir thoroughly for 1 hour to prepare dispersion B;
[0023] (4) Mix the mixed liquid A and the dispersion liquid B thoroughly and stir for 30 minutes to prepare a ...
Embodiment 2
[0025] A method for preparing sulfur fixation catalyst, the specific raw materials and methods are as follows:
[0026] (1) (1) Weigh parts by weight Weigh the following raw materials: 300 parts of water, 280 parts of glycerol, 125 parts of sodium carbonate, 140 parts of sodium methacrylate sulfonate, 200 parts of sodium gluconate, 135 parts of titanium dioxide, triethanolamine 75 copies.
[0027] (2) Add sodium carbonate, sodium methacrylate sulfonate, and sodium gluconate to 3 / 4 of the water, and stir well for 50 hours with a stirring tank to prepare mixed solution A;
[0028] (3) Add titanium dioxide to the remaining 1 / 4 of the water and stir for 35 minutes with a stirring tank, then add glycerol and triethanolamine and stir well for 70 hours to prepare dispersion B;
[0029] (4) Mix the mixed liquid A and the dispersion liquid B thoroughly and stir for 25 minutes to prepare a solid sulfur catalyst.
Embodiment 3
[0031] A method for preparing sulfur fixation catalyst, the specific raw materials and methods are as follows:
[0032] (1) 350 parts of water, 300 parts of glycerol, 115 parts of sodium carbonate, 150 parts of sodium methacrylate sulfonate, 160 parts of sodium gluconate, 180 parts of titanium dioxide, 80 parts of triethanolamine.
[0033] (2) Add sodium carbonate, sodium methacrylate sulfonate, and sodium gluconate to 3 / 4 of the water, and stir well for 70 hours with a stirring tank to prepare mixed solution A;
[0034] (3) Add titanium dioxide to the remaining 1 / 4 of the water and stir for 25 minutes in a stirring tank, then add glycerol and triethanolamine and stir well for 50 hours to prepare dispersion B;
[0035] (4) Mix the mixed liquid A and the dispersion liquid B fully and stir for 35 minutes to prepare a solid sulfur catalyst.
PUM
Property | Measurement | Unit |
---|---|---|
ignition point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com