Embodiment 1
[0020] A finishing process for upper garment fabrics, comprising the steps of:
[0021] 1) Put 1-2 parts by weight of N-acyl amino acid salt, 1.4 parts by weight of chitin, 0.9 parts by weight of catechol, and 0.4 parts by weight of natamycin into 20 parts by weight of deionized water in sequence, and stir evenly;
[0022] 2) Add 1.4 parts by weight of valerythrin, 1.3 parts by weight of hexabromocyclododecane, 0.7 parts by weight of fatty acid amine, and 1.4 parts by weight of diethylenetriamine at the same time, and continue to stir until fully mixed evenly to obtain a finishing liquid;
[0023] 3) Pad the fabric in the finishing solution, take it out and dry it at a constant temperature.
Embodiment 2
[0025] The finishing process of the upper garment fabric comprises the following steps:
[0026] 1) Put 1 part by weight of N-acyl amino acid salt, 1.4 part by weight of chitin, 0.9 part by weight of catechol, and 0.4 part by weight of natamycin into 20 parts by weight of deionized water, and stir evenly;
[0027] 2) Add 1.4 parts by weight of valerythrin, 1.3 parts by weight of hexabromocyclododecane, 0.7 parts by weight of fatty acid amine, and 1.4 parts by weight of diethylenetriamine at the same time, and continue to stir until fully mixed evenly to obtain a finishing liquid;
[0028] 3) Pad the fabric in the finishing solution, take it out and dry it at a constant temperature.
Embodiment 3
[0030] The finishing process of the upper garment fabric comprises the following steps:
[0031] 1) Put 2 parts by weight of N-acyl amino acid salt, 1.4 parts by weight of chitin, 0.9 parts by weight of catechol, and 0.4 parts by weight of natamycin into 20 parts by weight of deionized water in sequence, and stir evenly;
[0032] 2) Add 1.4 parts by weight of valerythrin, 1.3 parts by weight of hexabromocyclododecane, 0.7 parts by weight of fatty acid amine, and 1.4 parts by weight of diethylenetriamine at the same time, and continue to stir until fully mixed evenly to obtain a finishing liquid;
[0033] 3) Pad the fabric in the finishing solution, take it out and dry it at a constant temperature.