A preparation method and feed technology, applied in animal feed, animal feed, applications, etc., can solve the problems of feed easily becoming mushy, affecting the taste of catfish, and harming, so as to improve the body's ability and anti-cancer ability, and increase human immunity Power, reduce product cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A catfish feed rich in zinc and a preparation method thereof, the formula is: 15 parts by weight of flour, 15 parts by weight of peanut meal, 15 parts by weight of rice bran, 10 parts by weight of shrimp powder, 3 parts by weight of squid powder, and 3 parts by weight of pig liver powder part, 3 parts by weight of soybean flour. Its preparation process is: according to the raw material formula, various ingredients are mixed and crushed in proportion, and after being sieved through a 3.5mm sieve, the 2 Under steam pressure, tempering at 80°C for 100 seconds; then, use the feeder to make the pulverized powder material under the extrusion force of the die and roller to obtain a certain temperature and humidity, close to each other And the rearranged pellet feed, the commonly used die thickness is 45mm, the die aperture is 4.5mm; and then the pressure is 3kg / cm 2 , 3% of the steam heating slaking, 1.5 hours of slaking time, temperature 80 ℃, cooling, packaging to obtain th...
Embodiment 2
[0022] A catfish feed rich in zinc and a preparation method thereof, the formula is: 20 parts by weight of flour, 20 parts by weight of peanut meal, 20 parts by weight of rice bran, 15 parts by weight of shrimp meal, 7 parts by weight of squid meal, and 7 parts by weight of pig liver meal part, 10 parts by weight of soybean flour. Its preparation process is: according to the raw material formula, various ingredients are mixed and crushed in proportion, and after being sieved through a 3.5mm sieve, the 2 Under steam pressure, tempering at 80°C for 100 seconds; then, use the feeder to make the pulverized powder material under the extrusion force of the die and roller to obtain a certain temperature and humidity, close to each other And the rearranged pellet feed, the commonly used die thickness is 45mm, the die aperture is 4.5mm; and then the pressure is 3kg / cm 2 , 3% of the steam heating slaking, 1.5 hours of slaking time, temperature 80 ℃, cooling, packaging to obtain the fee...