Environment-friendly color fading resisting agent
An anti-fading, environment-friendly technology, applied in dyeing, textiles and papermaking, etc., can solve the problems of nylon fabrics with poor washing fastness, wet and dry rubbing fastness, perspiration fastness, and acid dyes' light fastness. Advanced problems, to achieve the effect of small chemical hazards and increase the vividness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] An environment-friendly anti-fading agent, the anti-fading agent comprises the following components by weight:
[0021] 3 parts sodium silicate;
[0022] 10 parts of phenol;
[0023] 12 parts of phenolsulfonic acid;
[0024] 7 parts of composite catalyst;
[0025] 12 parts of salt water;
[0026] 7 parts silkworm cocoons;
[0027] Modifier 2 parts.
[0028] The composite catalyst is a mixture of potassium hydroxide and boric acid.
[0029] Soak silkworm cocoons in warm water for 1 hour, the outer layer of silk of the soaked silkworm cocoons will be adjusted, and then become silkworm cocoons.
Embodiment 2
[0032] An environment-friendly anti-fading agent, the anti-fading agent comprises the following components by weight:
[0033] 5 parts of sodium silicate;
[0034] 15 parts of phenol;
[0035] 13 parts of phenolsulfonic acid;
[0036] 8 parts of composite catalyst;
[0037] 15 parts of salt water;
[0038] 8 parts silkworm cocoons;
[0039] Modifier 3 parts.
[0040] The composite catalyst is a mixture of potassium hydroxide and boric acid.
[0041] Soak silkworm cocoons in warm water for 1.5 hours. After soaking, a layer of silk outside the silkworm cocoons will be drawn and turned into cocoon silk.
Embodiment 3
[0044] An environment-friendly anti-fading agent, the anti-fading agent comprises the following components by weight:
[0045] 7 parts of sodium silicate;
[0046] 20 parts of phenol;
[0047] 15 parts of phenolsulfonic acid;
[0048] 9 parts of composite catalyst;
[0049] 18 parts of salt water;
[0050] 11 parts of cocoon silk;
[0051] Modifier 4 parts.
[0052] The composite catalyst is a mixture of potassium hydroxide and boric acid.
[0053] Soak silkworm cocoons in warm water for 2 hours. After soaking, a layer of silk on the outside of silkworm cocoons is drawn, and then becomes cocoon silk.
[0054] The modifier is urea or hydrogen peroxide.
[0055] The anti-fading agent in the present invention adopts phenol, phenol sulfonic acid and composite catalyst to undergo condensation reaction, and adds a modifier for modification to obtain an acid-resisting anti-fading agent. The chemical hazard is small, and salt water has a certain color fixation effect on fabrics...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com