A kind of tuff stone powder admixture for concrete and preparation method thereof
A technology of tuff and admixture, which is applied in the field of building materials, can solve the problems that the grinding efficiency of materials cannot be effectively improved, and the development and application of tuff has not attracted attention, so as to alleviate the situation of material supply, improve early volume stability, and reduce shrinkage cracks Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach
[0039] A preparation method for a tuff rock powder admixture for concrete, comprising the following steps in sequence:
[0040] Take 1000 parts by weight of tuff, add a modifier with a total amount of 0.13 to 1.3 parts by weight, and grind for 10 to 50 minutes to obtain a tuff powder admixture; check whether the performance index of the tuff powder admixture meets the specific surface area ≥ 300m 2 / kg, apparent density ρ≥2.64g / cm 3 ; If it meets the requirements, the finished product of tuff rock powder admixture is obtained; if it does not meet the requirements, it is discarded;
[0041] The modifier is prepared from a grinding aid component, an air-entraining component and a thickening component in a mass ratio of 10:1:2; the grinding aid component is triethanolamine, modified triethanolamine and triethanolamine One or any combination of two or three of isopropanolamines;
[0042]The air-entraining component is one or any combination of saponin air-entraining agents and ...
Embodiment 1
[0049] Get 1 part by weight of tuff ore debris, add 10 parts by weight of modified triethanolamine, 1 part by weight of triterpene saponin air-entraining agent, and modified xanthan gum of 2 parts by weight, and grind for 10 minutes , the obtained tuff rock powder admixture has a density of 2.65g / cm 3 , the specific surface area is 350.1m 2 / kg.
Embodiment 2
[0051] Get 1 part by weight of tuff ore debris, add 1 / 10,000 parts by weight of triethanolamine, 0.1 parts by weight of sodium dodecylbenzenesulfonate air-entraining agent, 0.1 parts by weight of modified xanthan gum, 0.1 parts by weight of hydroxypropyl methyl cellulose ether, grinding 50min, the obtained tuff rock powder admixture, the density is 2.66g / cm 3 , the specific surface area is 805.9m 2 / kg.
PUM
| Property | Measurement | Unit |
|---|---|---|
| specific surface area | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
| particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information