Waterproof board for anti-backflow automobile exhaust pipe device
A technology of automobile exhaust and waterproof board, which is applied in the direction of exhaust device, noise reduction device, application, etc., can solve the problems of backflow into the exhaust pipe, etc., and achieve the effect of ensuring quality, ensuring waterproof effect, and high production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] Such as Figure 1 to Figure 2 As shown, the present invention provides an anti-backflow automobile exhaust pipe device, comprising an air intake pipe 1, a lumen 2 communicated with the air intake pipe 1, and an outlet pipe 3 communicated with the lumen 2, and automobile exhaust enters the lumen from the air intake pipe 1 2 and discharged from the outlet pipe 3.
[0025] Specifically, a pneumatic valve 6 is provided on the wall of the lumen 2; a waterproof plate 4 that is oppositely arranged and connected to the air outlet pipe 3 is provided inside the outlet pipe 3; a stopper is provided on the side of the waterproof plate 4 near the lumen 2 5. The diameters of the air intake pipe 1 and the air outlet pipe 3 are equal. The diameter of the lumen 2 is greater than the diameters of the inlet pipe 1 and the outlet pipe 3 .
[0026] When encountering rainy weather or passing through a waterlogged road section, when there is accumulated water flowing into the air outlet pi...
Embodiment 2
[0029] Waterproof board for anti-backflow automobile exhaust pipe device, made of ethylene-vinyl acetate copolymer 30%, polyvinyl chloride 30%, polystyrene 20%, polyurethane 5%, graphite 5%, phenolic resin 5%, β-sitosterol 1% and antioxidant 4%.
Embodiment 3
[0031] A method for processing a waterproof plate for an anti-backflow automobile exhaust pipe device comprises the following steps:
[0032] (1) batching: take raw material by weight percentage of embodiment 2;
[0033] (2) Mixing: Stir and mix the raw materials, the mixing temperature is 90°C, and the stirring time is 5 minutes;
[0034] (3) Blending extrusion, the temperature of the screw rod of the extruder in the feeding section, the melting section, and the metering section is respectively 120°C, 180°C, and 160°C.
[0035] (4) Forming: The extruded material is calendered and formed with a three-roll calender, and the temperatures of the three rolls are 50°C, 60°C, and 70°C respectively;
[0036] (5) Air cooling to obtain finished products.