A formaldehyde scavenger, formaldehyde scavenger technology, applied in the field of indoor air purification, can solve the problems of low formaldehyde removal rate, complex preparation process, secondary pollution, etc., and achieve the effect of simple preparation process, low cost, and no secondary pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0022] A kind of preparation method of negative ion formaldehyde eliminating agent, comprises the following steps:
[0023] Step 1. Pour water into the dispersing kettle, start stirring and then add polyvinylpyrrolidone. After the polyvinylpyrrolidone is completely dissolved, slowly add magnesium aluminum silicate and disperse with a disperser for 10 to 30 minutes;
[0024] Step 2. Slowly add negative ion powder into the dispersing kettle in step 1, adjust the speed of the disperser to 1500r / min to 3000r / min, and continue to disperse with the disperser for 20min to 50min;
[0025] Step 3: sequentially add anhydrous sodium sulfite, sodium bisulfite, glycerin and propylene glycol into the dispersing kettle in step 2, and continue to disperse and stir for 20 to 50 minutes to obtain the final product.
[0026] The final product obtained is a liquid spray, which is easy to use; when in use, just spray the formaldehyde remover into the air, and after spraying in the air, the formald...
Embodiment 1
[0028] A kind of negative ion formaldehyde scavenger, it is made up of the raw material of following percentage by weight:
[0029] Polyvinylpyrrolidone 1%
[0030] Anhydrous sodium sulfite 8%
[0032] Propylene Glycol 2%
[0033] Glycerin 10%
[0034] Negative ion powder 5%
[0035] Magnesium Aluminum Silicate 3%
[0036] Water 70%.
[0037] Prepared according to the following steps:
[0038] Step 1. Pour 70% of the water into the dispersing tank, start stirring and then add 1% polyvinylpyrrolidone. After the polyvinylpyrrolidone is completely dissolved, slowly add 3% magnesium aluminum silicate and disperse for 10 minutes;
[0039] Step 2. Slowly add 5% negative ion powder into the dispersion kettle in step 1, adjust the speed of the disperser to 2500r / min, and disperse for 25 minutes;
[0040] Step 3, sequentially add 8% anhydrous sodium sulfite, 1% sodium bisulfite, 10% glycerin and 2% propylene glycol to the dispersion kettle in step 2...
Embodiment 2
[0042] A kind of negative ion formaldehyde scavenger, it is made up of the raw material of following percentage by weight:
[0043] Polyvinylpyrrolidone 3%
[0044] Anhydrous sodium sulfite 12%
[0046] Propylene Glycol 5%
[0047] Glycerin 15%
[0048] Negative ion powder 7%
[0049] Magnesium Aluminum Silicate 5%
[0050] Water 50%.
[0051] Prepared according to the following steps:
[0052] Step 1. Pour 50% of water into the dispersion tank, start stirring and then add 3% polyvinylpyrrolidone. After the polyvinylpyrrolidone is completely dissolved, slowly add 5% magnesium aluminum silicate and disperse for 15 minutes;
[0053] Step 2. Slowly add 7% negative ion powder into the dispersion kettle in step 1, adjust the speed of the disperser to 2000r / min, and disperse for 30 minutes;
[0054] Step 3, sequentially add 12% anhydrous sodium sulfite, 3% sodium bisulfite, 15% glycerin and 5% propylene glycol to the dispersion kettle in step 2, ...