An aging-resistant and environmentally friendly technology, applied in coatings and other directions, can solve problems such as water resistance and poor firmness, air pollution, and health hazards, and achieve excellent waterproof performance, high surface tension, and the effect of improving the color of the coating
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A healthy, environment-friendly, aging-resistant indoor wall paint, the raw materials include: 50 parts of composite ferric oxide microspheres, 10 parts of negative ion powder, 60 parts of tourmaline powder, 15 parts of diatomaceous earth, 25 parts of chrysotile , 2 parts of cement expanded perlite, 10 parts of quartz powder, 1 part of calcined clay, 40 parts of acrylate and styrene copolymer powder, 100 parts of water.
Embodiment 2
[0020] A healthy, environment-friendly, aging-resistant indoor wall coating, the raw materials of which include by weight: 20 parts of composite ferric oxide microspheres, 60 parts of negative ion powder, 10 parts of tourmaline powder, 50 parts of diatomaceous earth, 2 parts of chrysotile , 20 parts of cement expanded perlite, 1 part of quartz powder, 12 parts of calcined clay, 20 parts of acrylate and styrene copolymer powder, 150 parts of water.
Embodiment 3
[0022] A healthy, environment-friendly, aging-resistant indoor wall coating, the raw materials of which include by weight: 30 parts of composite ferric oxide microspheres, 30 parts of negative ion powder, 20 parts of tourmaline powder, 30 parts of diatomaceous earth, 10 parts of chrysotile , 15 parts of cement expanded perlite, 5 parts of quartz powder, 10 parts of calcined clay, 35 parts of acrylate and styrene copolymer powder, 140 parts of water.
[0023] Composite ferric oxide microspheres are prepared by the following process: take 10 parts by weight of FeCl 2 4H 2 O, 25 parts of FeCl 3 ·6H 2 O, 100 parts of deionized water, mixed evenly under the protection of nitrogen, heated up to 90 ° C, added 5 parts of NH3·H2O aqueous solution with a concentration of 0.5mol / L under stirring, the stirring speed was 300r / min, and magnetically separated to obtain Add 200 parts of Na at pH 11.6 to the solid 2 SiO 3 Ultrasonic dispersion of the solution, heating up to 70°C, adding h...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com