A processing method of wicker for improving the yield of woven products
A processing method and a technology of yield rate, applied in the field of wicker processing, can solve the problems of shortening the service life of willow products, reducing the quality of willow products, and reducing the service cycle, so as to improve the anti-cracking performance, enhance flexibility, and improve flexibility. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A method for processing wicker for improving the finished product rate of woven products, comprising the following steps:
[0020] (1) After the wicker is harvested, the leaves are removed, and the wicker is soaked in a sodium acetate solution with a mass fraction of 1.2% for 0.75h, and then soaked in a potassium sulfate solution with a mass fraction of 2% for 1.2h;
[0021] (2) Wrap the wicker processed in step (1) with mixed mud. The thickness of the mixed mud is 1.3cm, and then bake at 51°C for 1.5h. During the baking process, keep the baking evenly everywhere. Quickly soak the baked wicker wrapped in mixed mud in the treatment solution at a temperature of 30°C for 22 minutes;
[0022] (3) After cleaning the wicker treated in step (2), dry it at 44°C until the water content is 38%, and weave it; h, and then dried until the water content is 34%, the soaking solution is made of the following ingredients by weight: 6.5 parts of urea, 2.4 parts of sodium acetate, 1 part...
Embodiment 2
[0026] A method for processing wicker for improving the finished product rate of woven products, comprising the following steps:
[0027] (1) After the wicker is harvested, the leaves are removed, and the wicker is soaked in a sodium acetate solution with a mass fraction of 1.2% for 0.75h, and then soaked in a potassium sulfate solution with a mass fraction of 2% for 1.2h;
[0028] (2) Wrap the wicker processed in step (1) with mixed mud. The thickness of the mixed mud is 1.3cm, and then bake at 51°C for 1.5h. During the baking process, keep the baking evenly everywhere. Quickly soak the baked wicker wrapped in mixed mud in the treatment solution at a temperature of 30°C for 22 minutes;
[0029] (3) Wash the wicker treated in step (2) and dry it at 44°C until the moisture content is 38%, and weave it.
[0030] The mixed mud is prepared by mixing the following raw materials by weight: 38 parts of yellow clay, 0.32 parts of copper sulfate, 1.4 parts of lignocellulose, 9 parts o...
Embodiment 3
[0033] A method for processing wicker for improving the finished product rate of woven products, comprising the following steps:
[0034] (1) After the wicker is harvested, the leaves are removed, and the wicker is soaked in a sodium acetate solution with a mass fraction of 1.2% for 0.6h, and then soaked in a potassium sulfate solution with a mass fraction of 2% for 1.2h;
[0035] (2) Wrap the wicker processed in step (1) with mixed mud. The thickness of the mixed mud is 1cm, and then bake at 51°C for 1.2h. Soak the baked wicker wrapped in the mixed mud in the treatment solution at a temperature of 32°C for 28 minutes;
[0036] The mixed mud is made by mixing the following raw materials by weight: 36 parts of yellow clay, 0.36 parts of copper sulfate, 1.3 parts of lignocellulose, 10 parts of ginger juice, 3 parts of lemon juice, 5.2 parts of plant ash, and 22 parts of water;
[0037] The treatment solution is made of the following raw materials by weight: 2.8 parts of sodium ...
PUM
Login to View More Abstract
Description
Claims
Application Information