Condenser for automobile
A technology for condensers and automobiles, which is applied to evaporators/condensers, refrigerators, refrigeration components, etc., and can solve the problems of performance degradation of lightweight condensers in terms of corrosion resistance, weldability, shock resistance, etc. The effect of improvement, simple production process and high production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The automobile condenser provided by Embodiment 1 of the present invention includes a heat sink, and the heat sink includes an inner layer and a cladding layer coated on both sides of the inner layer; 13%~16%; the inner layer is made of aluminum alloy, containing 0.55~0.59mass% silicon, 0.65~0.69mass% iron, 0.25~0.3mass% copper, 1.55~1.6mass% manganese, 1.1~ 1.4mass% zinc, 0.3mass% zirconium, no more than 0.15mass% impurities, and the balance is aluminum; the cladding layer is made of aluminum alloy, containing 4.5-5.8mass% silicon, 0.3-0.7mass% iron , 0.1-0.2mass% copper, 0.01-0.04mass% manganese, 0.01-0.04mass% magnesium, 1.1-1.2mass% zinc, 0.16-0.19mass% titanium, no more than 0.15mass% impurities, other The amount is aluminum.
[0016] Manganese is added to the inner layer, and the manganese content reaches the solid solution limit, which greatly improves the strength of the heat sink; at the same time, the high content of zinc can reduce the corrosion potential of...
Embodiment 2
[0021] The automobile condenser provided by Embodiment 2 of the present invention includes a heat sink, and the heat sink includes an inner layer and a cladding layer coated on both sides of the inner layer; 14%; the inner layer is made of aluminum alloy, containing 0.56mass% silicon, 0.66mass% iron, 0.27mass% copper, 1.58mass% manganese, 1.25mass% zinc, 0.3mass% zirconium, not More than 0.15mass% impurities, the balance is aluminum; the cladding layer is made of aluminum alloy, containing 4.7mass% silicon, 0.5mass% iron, 0.15mass% copper, 0.03mass% manganese, 0.02mass% Magnesium, 1.15mass% of zinc, 0.17mass% of titanium, no more than 0.15mass% of impurities, and the balance of aluminum.
[0022] Using the automotive condenser provided in Example 2 of the present invention, the heat sink can achieve better corrosion resistance, castability, easy welding, high damping, and shockproof effects, while meeting the lightweight requirements of the condenser, all aspects of performanc...