A processing technology and signage technology, which is applied to the processing technology field of imitation silver signs, can solve the problems of different thicknesses of baking paint surface coatings, mixed decorative effects, and serrations, etc., and achieves good economic benefits, good decorative effects, and good flatness. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] Embodiment 1: A kind of processing technology of imitating silver signboard, it is characterized in that, comprises the following steps to finish:
[0021] Step 1. Remove the dust from the white carcass of the formed process sign, so that there are no maggot holes and sand spots on the surface, and at the same time dry the whole white carcass with a hot air blower;
[0022] Step 2. Put the finished white carcass on the paint spray rack, and evenly spray the diluted black paint to form a base color body. After the base color body dries, it is ready for use.
[0023] Step 3. Prepare gold ink by mixing gold oil and silver gold powder at a ratio of 1:1.
[0024] Step 4. Dip a little gold ink with a pig hair brush, rub it on the palette a few times, so that the gold ink is evenly mixed on the brush, and brush it on the background color body. The protruding part of the pig hair brush touches the gold ink and becomes golden , the concave part of the pig hair brush is still bl...
Embodiment 2
[0026] Embodiment 2, a processing method of imitation silver drawing process sign, is characterized in that, comprises the following steps to complete:
[0027] Step 1. Use No. 360 sandpaper to smooth the bottom plate,
[0028] Step 2. Spray epoxy primer evenly on the bottom plate,
[0029] Step 3. After spraying the primer, place it in an oven at 80-90°C and bake for 30-40 minutes.
[0030] Step 4. After cooling, spray the imitation silver primer, and then bake in an oven at 80-90°C for 30-40 minutes.
[0031] Step 5. After cooling, spray brushed imitation silver black paint,
[0032] Step 6. After the surface is leveled, use the drawing cloth fixed in the drawing fixture to carry out water milling in the same direction. After water milling for 30 minutes, the drawing is formed.
[0033] Step 7. Scrub the surface of the brushed bottom plate with clean water, spray matte varnish after the water is dry, and bake in the oven for 5 minutes.
[0034] The processing method usin...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com