Concrete water reducing agent and preparation method thereof
A concrete water reducer and retarder technology, applied in the field of concrete additives, can solve the problems of poor plasticizing effect, single performance, poor water reducing performance, etc., to improve crack resistance, compressive and flexural resistance, and improve bleeding Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] A concrete water reducer, which is made by mixing the following raw materials in parts by weight:
[0033] 20 parts melamine
[0034] 13 parts of sulfamic acid
[0035] 4 parts acrylamide
[0036] Sodium carboxymethyl cellulose 1 part
[0037] 5 parts ferrous sulfate
[0038] Methanol 10 parts
[0039] Animal waste hair hydrolyzate 3 parts
[0040] Sodium Gluconate 20 parts
[0041] 2 parts aluminum sulfate
[0042] 40 parts of water.
[0043] A preparation method of concrete water reducer, comprising the steps of:
[0044] (1) Add melamine, sulfamic acid, acrylamide, sodium carboxymethylcellulose, ferrous sulfate, low-molecular alcohol and aluminum sulfate in the reaction kettle in sequence, heat and stir to 30°C, and keep warm for 20 minutes;
[0045] (2) Add retarder to the solution in step (1), keep the temperature at 30°C, keep stirring for 30 minutes, add air-entraining agent to the solution, and stir for 30 minutes;
[0046] (3) Add water to the solutio...
Embodiment 2
[0048] A concrete water reducer, which is made by mixing the following raw materials in parts by weight:
[0049] 30 parts melamine
[0050] 15 parts of sulfamic acid
[0051] 2 parts acrylamide
[0052] Sodium carboxymethyl cellulose 3 parts
[0053] 1 part ferrous sulfate
[0054] Ethylene glycol 5 parts
[0055] Sodium dodecylbenzene sulfonate 7 parts
[0056] Sodium Gluconate 10 parts
[0057] 4 parts aluminum sulfate
[0058] 20 parts of water.
[0059] A preparation method of concrete water reducer, comprising the steps of:
[0060] (1) Add melamine, sulfamic acid, acrylamide, sodium carboxymethyl cellulose, ferrous sulfate, low molecular weight alcohol and aluminum sulfate in the reaction kettle in sequence, heat and stir to 50°C, and keep warm for 20 minutes;
[0061] (2) Add retarder to the solution in step (1), keep the temperature at 50°C, keep stirring for 30 minutes, add air-entraining agent to the solution, and stir for 30 minutes;
[0062] (3) Add wate...
Embodiment 3
[0064] A concrete water reducer, which is made by mixing the following raw materials in parts by weight:
[0065] 40 parts of melamine
[0066] 10 parts of sulfamic acid
[0067] 3 parts acrylamide
[0068] Sodium carboxymethyl cellulose 5 parts
[0069] 3 parts ferrous sulfate
[0070] Glycerol v 15 parts
[0071] Air-entraining agent 10 parts
[0072] Sodium Gluconate 15 parts
[0073] Aluminum sulfate 5 parts
[0074] 50 parts of water.
[0075] Wherein, the air-entraining agent is a mixture of animal waste hair hydrolyzate and sodium dodecylbenzenesulfonate in a mass ratio of 1:2.
[0076] A preparation method of concrete water reducer, comprising the steps of:
[0077] (1) Add melamine, sulfamic acid, acrylamide, sodium carboxymethylcellulose, ferrous sulfate, low-molecular alcohol and aluminum sulfate in the reaction kettle in sequence, heat and stir to 60°C, and keep warm for 20 minutes;
[0078] (2) Add retarder to the solution in step (1), keep the temperatu...
PUM
Property | Measurement | Unit |
---|---|---|
Freezing point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com