Core-to-core pillow and producing method thereof
A production method and technology of pillows, which are applied in the direction of pillows, textiles, papermaking, fiber processing, etc., can solve the problems of fiber agglomeration, pillow collapse, easy deformation, etc., and achieve the effects of good air permeability, not easy to collapse, and good support
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0014] Embodiment 1: see figure 1 , a method for making a core-in-core pillow, comprising the following steps: Step 1, feeding: through a vacuum negative pressure suction device, PE particles or powder are transported to the feeding port 1 of an extruder; Step 2, extruding: The raw material forms a molten state in the extruder 2, and is extruded into the spinneret 3 through the screw, and the heating temperature is controlled at 150°C, and the extrusion pressure is 2Mpa; Step 3, spinning: the raw material located in the spinneret 3 is under pressure Continuously extrude from the spinneret hole at the lower end of the spinneret 3, the spinneret hole diameter is 0.3mm, and the spinneret hole spacing is 0.4mm; Step 4, forming: the cooling forming device performs continuous circular motion, and the internal setting There are a first water area 41 and a second water area 42. The first water area 41 is provided with a first forming roller 411 moving in opposite directions and a firs...
Embodiment 2
[0016] Example 2: see figure 1, a method for making a core-in-core pillow, comprising the following steps: Step 1, feeding: through a vacuum negative pressure suction device, the particles or powders mixed with PE and POE are transported to the feeding port 1 of the extruder; the steps 2. Extrusion: The raw material forms a molten state in the extruder 2, and is extruded into the spinneret 3 through the screw, and the heating temperature is controlled at 280°C, and the extrusion pressure is 20Mpa; Step 3, Spinning: located in the spinneret 3 The raw material is continuously extruded from the spinneret hole at the lower end of the spinneret 3 under pressure, the spinneret hole diameter is 1.2mm, and the spinneret hole spacing is 2mm; movement, and the first water area 41 and the second water area 42 are arranged inside, the first forming roller 411 and the first group of toothed traction rollers 421 moving opposite are arranged in the first water area 41, through The multiple ...