A technology of anti-corrosion and anti-mildew, phenolic resin, applied in the field of adhesives, can solve the problems of poor penetration, air pollution, inability to completely remove mold nutrients, etc., and achieve excellent anti-corrosion performance, long-lasting anti-corrosion performance, and good anti-corrosion and anti-mold performance. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0025] Resin preparation comprises the following steps:
[0026] (1) Add 40 parts by weight of 100% concentration of phenol solution to the reaction kettle, add one-fifth of 4 parts by weight of 50% concentration of sodium hydroxide solution, start stirring, and control the temperature below ;
[0027] (2) The above reaction solution is cooled below Below, add 1 / 4th of the 50% concentration formaldehyde solution of 40 parts by weight ratio of slow speed, control exothermic to , and in Keep warm for 30min;
[0028] (3) After the heat preservation is over, slowly add 40 parts by weight of 50% formaldehyde solution and the remaining three-quarters, finish adding within 30 minutes, and keep the temperature at ;
[0029] (4) in keep warm for 1 hour;
[0030] (5) At the end of the heat preservation, slowly add 4 parts of the remaining 4 / 5 of the 50% concentration sodium hydroxide solution of 4 parts by weight;