A technology of heavy metal ions and heavy metals, applied in chemical instruments and methods, water pollutants, multi-stage water treatment, etc., can solve the problems of increased burden, non-biodegradable pollutants, high cost, etc., and achieves wide application range and high removal efficiency High, simple effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] Water containing complexed heavy metal ions (Ni 2+ :155mg / L; Zn 2+ :50mg / L)
[0042] 1) Adjust the pH of the water body containing complexed heavy metal ions to 6 and react with the heavy metal replacement reagent sodium sulfide (12g / L). The reaction time is 3 hours, adjust the pH to 9, and then add an anionic polyacrylamide (25g / L tons of water);
[0043] 2) carry out Fenton reaction after step 1) gained supernatant is adjusted pH to 2, namely add hydrogen peroxide 6L / ton of water (hydrogen peroxide content 30%) and ferrous ion 8kg / ton of water (ferrous sulfate), the reaction time is 2 hours, then adjust the pH to 8.5 for precipitation;
[0044] 3) Adjust the pH of the supernatant obtained in step 2) to 5 and react with the heavy metal replacement reagent sodium sulfide 6g / L. After the reaction time is 3 hours, adjust the pH to 9, and then add the heavy metal scavenger anionic polyacrylamide 12g / ton water, to obtain the heavy metal ion content in the supernatant ...
Embodiment 2
[0046] Water containing complexed heavy metal ions (Ni 2+ :88mg / L; Zn 2+ :55mg / L; Pb 2+ :20mg / L)
[0047] 1) Adjust the pH of the water containing complexed heavy metal ions to 1 and react with the heavy metal replacement reagent sodium sulfite 5g / L. The reaction time is 2 hours, adjust the pH to 10, and then add the heavy metal scavenger neutral polyacrylamide 20g / ton of water;
[0048] 4) carry out Fenton reaction after step 1) gained supernatant is adjusted pH to 1, namely add hydrogen peroxide 10L / ton of water (hydrogen peroxide content 30%) and ferrous ion 3kg / ton of water (ferrous sulfate), the reaction time is 3 hours, then adjust the pH to 8.5 for precipitation;
[0049] 5) Adjust the pH of the supernatant obtained in step 2) to 4 and react with the heavy metal replacement reagent sodium sulfite 10g / L. The reaction time is 4 hours, adjust the pH to 9, and then add the heavy metal scavenger polyaluminum chloride 100g / ton of water to obtain The content of heavy met...
Embodiment 3
[0051] Water containing complexed heavy metal ions (Ni 2+ :205mg / L; Zn 2+ :89mg / L; Pb 2+ :18mg / L; Cu 2+ :50mg / L)
[0052] 1) Adjust the pH of the water containing complexed heavy metal ions to 5 and react with the heavy metal replacement reagent ferric chloride 25g / L. The reaction time is 3 hours, then adjust the pH to 8.5, and then add 50g / ton of heavy metal scavenger cationic polyacrylamide water;
[0053] 2) After adjusting the pH of the supernatant obtained in step 1) to 3, carry out the Fenton reaction, that is, add 20L / ton of hydrogen peroxide (hydrogen peroxide concentration is 30%) and 25kg / ton of ferrous ion water (ferrous sulfate), and the reaction time For 4 hours, then adjust the pH to 9 for precipitation;
[0054] 3) Adjust the pH of the supernatant obtained in step 2) to 3 and react with the heavy metal replacement reagent ferric chloride 15g / L. The reaction time is 3 hours, then adjust the pH to 9, and then add the heavy metal scavenger polyaluminium ferric...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com