Embodiment 1
[0023] Grind a certain copper sulfide ore to -0.074mm, accounting for 65%, add sulfuric acid as a regulator with a concentration of 5% to adjust the pH of the pulp to 5.5, add 2000g / t particle size to -0.010mm, the particle size content accounts for 85%, and the purity is 80% fine-grained serpentine minerals were mixed for 10 minutes, and then 300g / t calcium lignosulfonate, 100g / t butyl xanthate, and 20g / t No. 2 oil were added for rough separation of copper sulfide minerals , to obtain roughing concentrate and roughing tailings. Sodium hexametaphosphate is added to the roughing concentrate for twice beneficiation to obtain the final concentrate. The amount of sodium hexametaphosphate in beneficiation 1 is 400g / t, and the amount of sodium hexametaphosphate in beneficiation 2 is 200g / t. The mid-mine sequence returns to the previous level of operation. Add collector butyl xanthate and foaming agent No. 2 oil to the roughing tailings for two times of sweeping to obtain the final ...
Embodiment 2
[0027] Grind a certain copper sulfide ore to -0.074mm, accounting for 75%, add sulfuric acid as a regulator with a concentration of 8% to adjust the pH of the pulp to 6.8, add 6500g / t particle size to -0.010mm, the particle size content accounts for 95%, and the purity is 90% fine-grained serpentine minerals were mixed for 5 minutes, and then 500g / t calcium lignosulfonate, 120g / t butyl xanthate, and 30g / t No. 2 oil were added for rough separation of copper sulfide minerals , to obtain roughing concentrate and roughing tailings. Add trisodium phosphate to the rough concentrate to carry out twice beneficiation to obtain the final concentrate. The amount of beneficiation 1 trisodium phosphate is 400g / t, the amount of beneficiation 2 trisodium phosphate is 200g / t, and the beneficiation of middle ore Sequentially return to the previous job. Add the collector butyl xanthate and foaming agent No. 2 oil to the roughing tailings for two times of sweeping to obtain the final tailings. ...