Water treatment and cyclic utilization system
A water treatment and water pump technology, applied in the field of water source purification, can solve the problems of residual ozone and difficult cleaning of water treatment equipment, and achieve the effects of improving compatibility and dispersibility, excellent hydrophobicity and oleophobicity, and good water resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0043] The preparation method of the porous adsorption carrier is:
[0044] (1) the loofah vine is incinerated into ash, for subsequent use;
[0045] (2) Grinding the medical stone to a particle size of 325 mesh, placing it in a sodium hydroxide solution with a mass fraction of 20%, with a solid-to-liquid ratio of 1:20, stirring and reacting at 80°C for 30 minutes, washing with distilled water until neutral, Dried to obtain modified medical stone;
[0046] (3) Dissolve the gelatin in hot water, then add the medical stone and the ash of the loofah vine obtained in step (1), stir and mix evenly to obtain a gelatinous material, then add alcohol to precipitate the gelatin, filter to obtain the medical stone Composite sponge;
[0047] (4) Roasting the medical stone composite sponge body obtained in step (3) at a high temperature of 700° C. for 2 hours, after cooling down, grinding and pulverizing to 200 mesh to obtain medical stone composite powder;
[0048] (5) Put hydroxypropy...
Embodiment 1
[0053] The components of the polyurethane composite coating are in parts by mass: 40 parts of acrylic resin, 30 parts of polyurethane resin, 1 part of polydimethylsiloxane, 6 parts of nanocellulose, 0.5 parts of emulsifier, and 3 parts of fluorinated graphite , 4 parts of nano-silica, 6 parts of nano-titanium dioxide, 1 part of fluorosilane coupling agent, 30 parts of dichloromethane, 20 parts of acetone, 0.2 part of cocoic acid diethanolamide, 1 part of dodecyl alcohol ester, calcium carbonate 6 parts, 0.2 parts of leveling agent.
[0054] The preparation method of the polyurethane composite coating is as follows: adding fluorosilane coupling agent and polydimethylsiloxane into acetone, stirring and dispersing evenly, then adding nano-silica and nano-titanium dioxide and stirring for 2 hours, during the stirring process, every 0.5 h Add ultrasonic treatment, the power of ultrasonic treatment is 600W, the frequency is 140kHz, each time ultrasonic 10-15min, obtain mixed materia...
Embodiment 2
[0056] The components of the polyurethane composite coating in parts by mass are: 50 parts of acrylic resin, 35 parts of polyurethane resin, 1.5 parts of polydimethylsiloxane, 9 parts of nanocellulose, 0.8 parts of emulsifier, and 4 parts of graphite fluoride , 6 parts of nano-silicon dioxide, 8 parts of nano-titanium dioxide, 1.5 parts of fluorosilane coupling agent, 35 parts of dichloromethane, 25 parts of acetone, 0.6 part of coconut acid diethanolamide, 2 parts of dodecyl alcohol ester, calcium carbonate 7 parts, 0.5 parts of leveling agent.
[0057] The preparation method of the polyurethane composite coating is as follows: adding fluorosilane coupling agent and polydimethylsiloxane into acetone, stirring and dispersing evenly, then adding nano-silica and nano-titanium dioxide and stirring for 2 hours, during the stirring process, every 0.5 h Add ultrasonic treatment, the power of ultrasonic treatment is 700W, the frequency is 120kHz, each ultrasonic 10-15min, obtain mixe...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com