Unlock instant, AI-driven research and patent intelligence for your innovation.

A kind of preparation method of sofa leather

A leather and sofa technology, applied in the field of sofa leather preparation, can solve the problems of soft texture of sofa leather, affect the comfort of sofa use, reduce the service life of sofa, etc., achieve the effects of soft texture, improved aesthetics and guaranteed quality

Active Publication Date: 2020-09-08
安吉众合新材料科技有限公司
View PDF3 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

In the sofa manufacturing industry, sofa leather has been widely used; there are many kinds of sofa leather currently used, but after long-term use, it is found that the texture of sofa leather is not soft, and there will be aging and peeling of the skin, which will cause serious damage. Affect the comfort of the sofa itself, so that the service life of the sofa itself will be greatly reduced

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

preparation example Construction

[0008] What this application proposes is a preparation method of sofa leather, which includes the following steps: Step 1: select a whole piece of antelope skin, immerse the antelope skin in water with additives and stir it, and heat it during the stirring process. The heating temperature is 30 ℃~50℃, the stirring time is 1~3 hours; Step 2: take out the whole antelope skin, dry it in the air, wrap it with lime powder, then put the antelope skin wrapped in lime powder at a concentration of 20~50g / Soak in L of sodium sulfide solution for 5 to 10 hours; step three: depilate and expand, put the soaked antelope skin into a dehydrator for dehydration, and use a mechanical arm to take out the wool from the dehydrated antelope skin; step four: remove the processed antelope skin Put the antelope skin into water for heating, the heating temperature is 30°C-50°C, add 0.1%-0.3% hydrochloric acid, 1%-3% ammonium chloride into the water, soak for 1-2 hours, and adjust the pH to 8-3%. 10; S...

Embodiment 1

[0011] A method for preparing sofa leather, comprising the following steps: Step 1: select a whole piece of antelope skin, immerse the antelope skin in water added with additives and stir, and heat during the stirring process. The heating temperature is 30°C, and the stirring time is 1 hour; step 2: take out the whole antelope skin, dry it, wrap it with lime powder, and then soak the antelope skin wrapped in lime powder in a sodium sulfide solution with a concentration of 20 / L for 5 hours; step 3 : Depilation and expansion, put the soaked antelope skin into a dehydrator for dehydration, and use a mechanical arm to take out the wool from the dehydrated antelope skin; Step 4: Put the treated antelope skin into water for heating, the heating temperature is 3°C, Add 0.1% hydrochloric acid and 1% ammonium chloride to the water, soak for 1 hour, and adjust the pH to 8; Step 5: Put the processed antelope skin into water for heating at a temperature of 3°C, and add pancreas to the wate...

Embodiment 2

[0013] A method for preparing sofa leather, comprising the following steps: Step 1: select a whole piece of antelope skin, immerse the antelope skin in water added with additives and stir, and heat during the stirring process. The heating temperature is 40°C, and the stirring time is 2 hours; Step 2: Take out the whole antelope skin, dry it, wrap it with lime powder, and then soak the antelope skin wrapped in lime powder in a sodium sulfide solution with a concentration of 30g / L for 8 hours; Step 3 : Depilation and expansion, put the soaked antelope skin into a dehydrator for dehydration, and use a mechanical arm to take out the wool from the dehydrated antelope skin; Step 4: Put the treated antelope skin into water for heating, the heating temperature is 45°C, Add 0.2% hydrochloric acid and 2% ammonium chloride to the water, soak for 1.5 hours, and adjust the pH to 9; Step 5: put the treated antelope skin into water for heating, the heating temperature is 45°C, add pancreas to...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
concentrationaaaaaaaaaa
concentrationaaaaaaaaaa
concentrationaaaaaaaaaa
Login to View More

Abstract

The invention relates to the technical field of sofa leather, in particular to a preparation method for the sofa leather. The preparation method comprises the following steps of 1, soaking and heating; 2, wrapping ash alkali; 3, dehairing and expanding; 4, deashing; 5, softening; 6, acid leaching; 7, primary tanning; 8, retanning; 9, dyeing and fatting for the first time; 10, dyeing and fatting for the second time; 11, drying the treated goat skin of the antelope sheep, and spraying the surface layer; and 12, drying the sprayed the goat skin of the antelope sheep for 1-2 days to obtain a finished product. According to the preparation method for the sofa leather, the processing technology is simple, the prepared finished product is soft in texture, the wear resistance and the aging resistance are high, the service life is long, the quality of the sofa can be well guaranteed, the appearance attractiveness of the sofa can be improved, and the use comfort degree of the sofa can be improved.

Description

technical field [0001] The invention relates to the technical field of sofa leather, in particular to a preparation method of sofa leather. Background technique [0002] With the continuous development of society, the artificial leather industry has developed rapidly. In the sofa manufacturing industry, sofa leather has been widely used; there are many kinds of sofa leather currently used, but after long-term use, it is found that the texture of sofa leather is not soft, and there will be aging and peeling of the skin, which will cause serious damage. Affect the use comfort of sofa itself, make the service life of sofa itself also can reduce greatly. Contents of the invention [0003] The technical problem to be solved by the present invention is: in order to solve the problems existing in the prior art in the above-mentioned background technology, a preparation method of sofa leather is provided, the processing technology is simple, the finished product is soft in textur...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)