Embodiment 1
[0024] Example 1: Toxic side effects and biocompatibility of liquid metals
[0025] 1. Cell experiments
[0026] The cell verification experiment was carried out in accordance with the national standard GB / T16886.5 of the People's Republic of China (Medical Device Biological Evaluation Part 5: In vitro Cytotoxicity Test) and the relevant provisions of the International Medical Device Biological Evaluation Standard ISO10993-5, using mouse fibroblast L929 And human breast cancer cell MCF-7 as the research object, the in vitro biosafety evaluation of liquid metal was carried out.
[0027] Take 1mL of liquid metal for two days of ultraviolet sterilization, add 200μL of liquid metal to a 5ml EP tube, oscillate to make the liquid metal adhere to the tube wall and cover the entire bottom of the tube, remove excess liquid metal, add RPMI1640 basic culture medium, and make the liquid metal and liquid The surface area to volume ratio is 3 cm 2 / mL at 37°C, 5% CO 2 After 24 hours in t...
Embodiment 2
[0031] Embodiment 2: Preparation of drug-loaded liquid metal complex
[0032] The preparation process of the drug-loaded liquid metal complex is as follows: figure 1 As shown, it specifically includes the following steps:
[0033] (1) Preparation of drug-loaded silica: Prepare silica by template method, weigh 0.417g CTAB and 4.69g dodecylamine and add to a mixed solution of 180mL pure water, 300mL absolute ethanol and 20mL isopropanol, then Add 0.07mL of ammonia water and 15mL of tetraethyl orthosilicate, stir at 300r / min for 15min, then stir for 2h after observing that the solution becomes turbid, wash with ethanol for 3 times, dry or freeze-dry, sinter at 550K for 4h to remove the template agent, and obtain two silicon oxide. Take 20 mg of silicon dioxide and add it to a doxorubicin solution with a concentration of 2 mg / ml, and centrifuge to collect the lower precipitate to obtain drug-loaded silicon dioxide.
[0034] (2) Add 1 mL of liquid metal to the EP tube, then add ...
Embodiment 3
[0036] Embodiment 3: Preparation of drug-loaded liquid metal complex
[0037] (1) The difference from Example 2 is that 60 mg of silicon dioxide is added to a paclitaxel solution with a concentration of 2 mg / ml, and the solvent is volatilized to obtain drug-loaded silicon dioxide;
[0038] (2) The difference from Example 2 is that the surfactant is sorbitan, and 100 μL of sorbitan is added to 1 ml of liquid metal;
[0039] (3) Add 1 mL of liquid metal pellets to 60 mg of drug-loaded silica, and mix for 30 seconds at room temperature using a vortex mixer to obtain the drug-loaded liquid metal complex.
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com