Embodiment 1
[0031] A method for preparing an antibacterial mosquito repellent fiber fabric, comprising the following process steps:
[0032] (1) Preparation of mosquito repellent fiber: Mix 100 parts of water, 1 part of surfactant, 5 parts of oil-soluble essence, 8 parts of permethrin, and 50 parts of silica sol; heat to 80°C and stir 3h; immerse the artificial fiber in the above mixed solution, soak at room temperature for 12h, and then bake at 60°C for 20min to obtain the mosquito repellent fiber;
[0033] (2) Preparation of antibacterial fiber: immerse antibacterial fiber in nano-silver antibacterial solution, heat up to 42-46°C for 0.5-1h, then heat up to 65-75°C for 1-2h, then bake at 60-70°C for 3-5min , to obtain warp silk antibacterial fiber;
[0034] (3) The antibacterial fiber is used as the weft and the mosquito repellent fiber is used as the warp to weave an antibacterial and mosquito repellent layer;
[0035] (4) The antibacterial and mosquito repellent layer is fixed betwe...
Embodiment 2
[0037] A method for preparing an antibacterial mosquito repellent fiber fabric, comprising the following process steps:
[0038] (1) Preparation of mosquito repellent fiber: Mix 100 parts of water, 2 parts of surfactant, 3 parts of oil-soluble essence, 3 parts of permethrin, and 30 parts of silica sol; heat to 80°C and stir 3h; immerse the artificial fiber in the above mixed solution, soak at room temperature for 12h, and then bake at 60°C for 20min to obtain the mosquito repellent fiber;
[0039] (2) Preparation of antibacterial fiber: immerse antibacterial fiber in nano-silver antibacterial solution, heat up to 45°C for 1 hour, then heat up to 70°C for 2 hours, and then bake at 70°C for 15 minutes to obtain warp silk antibacterial fiber;
[0040] (3) The antibacterial fiber is used as the weft and the mosquito repellent fiber is used as the warp to weave an antibacterial and mosquito repellent layer;
[0041] (4) The antibacterial and mosquito repellent layer is fixed betwe...
Embodiment 3
[0043] A method for preparing an antibacterial mosquito repellent fiber fabric, comprising the following process steps:
[0044] (1) Preparation of mosquito repellent fiber: Mix 100 parts of water, 10 parts of surfactant, 15 parts of oil-soluble essence, 8 parts of permethrin, and 50 parts of silica sol in order; heat to 80°C and stir 3h; immerse the artificial fiber in the above mixed solution, soak at room temperature for 12h, and then bake at 60°C for 20min to obtain the mosquito repellent fiber;
[0045] (2) Preparation of antibacterial fiber: immerse antibacterial fiber in nano-silver antibacterial solution, heat up to 45°C for 1 hour, then heat up to 70°C for 2 hours, and then bake at 70°C for 15 minutes to obtain warp silk antibacterial fiber;
[0046] (3) The antibacterial fiber is used as the weft and the mosquito repellent fiber is used as the warp to weave an antibacterial and mosquito repellent layer;
[0047] (4) The antibacterial and mosquito repellent layer is ...