Preparation method and application of magnetic biological flocculant
A biological flocculant and magnetic technology, applied in chemical instruments and methods, biological water/sewage treatment, water pollutants, etc., can solve problems such as complex heavy metal ion methods, secondary pollution costs, and difficult product separation, achieving simple and fast Effect of separation and recovery, reduction of flocculation cost and improvement of flocculation efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0029] Specific implementation mode 1: This implementation mode is a preparation method of a magnetic bioflocculant, which is completed according to the following steps:
[0030] 1. Preparation of magnetic Fe 3 o 4 Particles:
[0031] FeCl 3 ·6H 2 O and FeSO 4 ·7H 2 Dissolve O into the solvent, heat it in a water bath to 85°C-95°C, then add ammonia water and distilled water with a mass fraction of 25% in sequence, stir and react at a temperature of 85°C-95°C for 20min-40min, then cool naturally to room temperature, and then Centrifuge to collect the black precipitate; use distilled water to wash the black precipitate until the washing solution is neutral to obtain the magnetic Fe 3 o 4 particles;
[0032] FeCl as described in step 1 3 ·6H 2 The volume ratio of the mass of O to the solvent is (6g~7g):100mL;
[0033] FeSO as described in step one 4 ·7H 2 The volume ratio of the mass of O to the solvent is (4g~5g):100mL;
[0034] The mass fraction described in step ...
specific Embodiment approach 2
[0058] Embodiment 2: The difference between this embodiment and Embodiment 1 is that the solvent described in step 1 is distilled water. Others are the same as in the first embodiment.
specific Embodiment approach 3
[0059] Specific embodiment three: the difference between this embodiment and specific embodiment one or two is: in step one, FeCl 3 ·6H 2 O and FeSO 4 ·7H 2 Dissolve O into the solvent, heat in a water bath to 85°C-90°C, then add ammonia water and distilled water with a mass fraction of 25% in sequence, stir and react at a temperature of 85°C-90°C for 20min-30min, then cool naturally to room temperature, and then Centrifuge to collect the black precipitate; use distilled water to wash the black precipitate until the washing solution is neutral to obtain the magnetic Fe 3 o 4 particles. Others are the same as in the first or second embodiment.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com