A technology of black copper and soldering sheet, applied in welding equipment, manufacturing tools, welding medium, etc., can solve problems such as unbearable stretching, peeling, tearing, depression, easy falling off of welding parts, and damage to silver patterns , to achieve the effect of docile flux, suitable welding temperature and improved efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] (1) Prepare materials according to the following components by mass:
[0028] 100 copies of silver powder,
[0029] 20 parts of copper,
[0030] 12 parts of zinc powder,
[0031] 3 parts table salt,
[0032] Arsenic (arsenic trioxide) 0.5 parts;
[0033] (2) Mix the components in step (1) and heat until they are melted into an alloy, and then beat the alloy into sheets to obtain solder sheets for black copper and silver production.
[0034] The obtained soldering sheet for the production of black copper and silver is used through the following steps:
[0035] a. According to the size of the black copper silver object to be welded, cut the solder piece into a small piece with a length of 2 mm, a width of 2 mm, and a thickness of 0.2 mm;
[0036] b. Mix borax and water at a solid-to-liquid mass ratio of 3:100, and stir and heat to obtain a mixed solution at 90°C;
[0037] c. Apply the mixture in step b to the weld joint or seam, then dip the small pieces in step a i...
Embodiment 2
[0039] (1) Prepare materials according to the following components by mass:
[0040] 100 copies of silver powder,
[0041] 15 parts of copper,
[0042] 10 parts of zinc powder,
[0043] 2 parts table salt,
[0044] Arsenic (arsenic trioxide) 0.2 parts;
[0045] (2) Mix the components in step (1) and heat until they are melted into an alloy, and then beat the alloy into sheets to obtain solder sheets for black copper and silver production.
[0046] The obtained soldering sheet for the production of black copper and silver is used through the following steps:
[0047] a. According to the size of the black copper silver object to be welded, cut the solder piece into a small piece with a length of 1 mm, a width of 1 mm, and a thickness of 0.1 mm;
[0048] b. Mix borax and water at a solid-to-liquid mass ratio of 2:100, and stir and heat to obtain a mixed solution at 100°C;
[0049] c. Apply the mixed solution in step b to the weld joint or seam, then dip the small piece in s...
Embodiment 3
[0051] (1) Prepare materials according to the following components by mass:
[0052] 100 copies of silver powder,
[0053] 25 parts of copper,
[0054] 15 parts of zinc powder,
[0055] 5 parts of table salt,
[0056] Arsenic (arsenic trioxide) 0.8 parts;
[0057] (2) After mixing the components in step (1), heat them until they are melted into an alloy, and then beat the alloy into sheets to obtain solder sheets for black copper and silver production.
[0058] The obtained soldering sheet for the production of black copper and silver is used through the following steps:
[0059] a. According to the size of the black copper silver object to be welded, cut the solder piece into a small piece with a length of 3 mm, a width of 3 mm, and a thickness of 0.5 mm;
[0060] b. Mix borax and water at a solid-to-liquid mass ratio of 5:100, and stir and heat to obtain a mixed solution at 80°C;
[0061] c. Apply the mixed solution in step b to the welding joint or seam, then dip the ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com