A manufacturing method and large-scale technology, applied in the field of musical instruments, can solve problems such as poor drum cavity reverberation, insufficient airtightness of the drum cavity, and influence on resonance, etc., and achieve the effects of dull drum body, good reverberation effect, and high resonance intensity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0039] A method for manufacturing a large drum, comprising the following steps:
[0040] Step 1. Soak peach wood and red cone wood in lime water for 1-2 days, then take them out and dry them in the sun; soak the sun-dried peach wood and red cone wood in water for 5 months, then take them out and dry them; The dry peach wood and red cone are burned to make a 1 cm carbonized layer on the wood surface, and the core material is obtained after removing the carbonized layer; the core material is cut into plates, then soaked in resin for 15 days and then dried to obtain dry peach wood and Dried red vertebra wood, sawing dry peach wood to grow 1.5 meters, wide 8 centimeters, thick 5 centimeters peach board, sawing dry red vertebra wood to grow 1.5 meters, wide 8 centimeters, thick 3 centimeters red vertebra board.
[0041] Step 2, mixing silica particles with a particle size of 50 microns and wood wax oil in a mass ratio of 1:10 to obtain an immersion liquid, placing the peach wood bo...
Embodiment 2
[0052] A method for manufacturing a large drum, comprising the following steps:
[0053] Step 1. Soak peach wood and red cone wood in lime water for 2 days, then take them out and dry them in the sun; soak the sun-dried peach trees and red cone wood in water for 6 months, then take them out and dry them again; Peach wood and red cone are carried out fire treatment, make the carbonized layer of 2 centimeters form on the wood surface, get core material after removing the carbonized layer; The core material is cut into plates, then placed in epoxy resin and soaked for 20 days and then dried to obtain dry peach wood and Dry red vertebral wood, the thickness of the peach wood board is 5 cm, and the width is 8 cm; the thickness of the red vertebral board is 3 cm, the width is 8 cm, and the length is 1.2 meters.
[0054] Step 2, mixing silica particles with a particle size of 0 microns and wood wax oil in a mass ratio of 1:10 to obtain an immersion solution, placing the peach wood bo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com