A technology for ecological environment and lake water, applied in chemical instruments and methods, water pollutants, adsorbed water/sewage treatment, etc., can solve problems such as high cost of reagents and equipment, high difficulty in recovery, complicated and lengthy operation process, etc., to achieve guaranteed Effect of water quality, cost saving, good adsorption performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0046] A lake water eco-environment restoration method comprises the steps of dividing the lake into several blocks with partitions, and then putting carbon aerogel A and nano film B into the blocks and reacting for 12 hours.
[0047] The mass-to-volume ratio of the dosage of carbon airgel A to the amount of treated water is 0.5 g / L. The mass-to-volume ratio of the dosage of the nano-film B to the amount of treated water is 0.5 g / L.
[0048] The preparation method of carbon airgel A:
[0049] (1) Mix 50 parts of formaldehyde and 25 parts of melamine, stir at 100 rpm, add triethanolamine dropwise until the pH value is 9.5, connect it to a reflux condenser and heat to 60°C, after heating for 30 minutes, a prepolymer solution is obtained.
[0050] (2) Dissolve 1 part of lignin in 20 parts of pure water and prepolymer solution, then add 37%wt ammonia water to adjust the pH of the solution to 11, stir at 50rpm for 10min, add 0.1mol / L hydrochloric acid dropwise to adjust the pH of ...
Embodiment 2
[0059] A lake water eco-environment restoration method comprises the steps of dividing the lake into several blocks with partitions, and then putting carbon aerogel A and nano film B into the blocks and reacting for 12 hours.
[0060] The mass-to-volume ratio of the dosage of carbon airgel A to the amount of treated water is 5g / L. The mass-to-volume ratio of the dosage of nano-film B to the amount of treated water is 5g / L.
[0061] The preparation method of carbon airgel A:
[0062] (1) Mix 50 parts of formaldehyde and 25 parts of melamine, stir at 100 rpm, add triethanolamine dropwise until the pH value is 9.5, connect it to a reflux condenser and heat to 60°C, after heating for 30 minutes, a prepolymer solution is obtained.
[0063] (2) Dissolve 1 part of lignin in 20 parts of pure water and prepolymer solution, then add 37%wt ammonia water to adjust the pH of the solution to 11, stir at 50rpm for 10min, add 0.1mol / L hydrochloric acid dropwise to adjust the pH of the soluti...
Embodiment 3
[0072] A lake water eco-environment restoration method comprises the steps of dividing the lake into several blocks with partitions, and then putting carbon airgel A and nano film B into the blocks for 24 hours of reaction.
[0073] The mass-to-volume ratio of the dosage of carbon airgel A to the amount of treated water is 0.5 g / L. The mass-to-volume ratio of the dosage of the nano-film B to the amount of treated water is 0.5 g / L.
[0074] The preparation method of carbon airgel A:
[0075] (1) Mix 100 parts of formaldehyde and 50 parts of melamine, stir at 100 rpm, add triethanolamine dropwise until the pH value is 9.5, connect to a reflux condenser and heat to 60°C, and after heating for 30 minutes, a prepolymer solution is obtained.
[0076] (2) Dissolve 10 parts of lignin in 20 parts of pure water and prepolymer solution, then add 37%wt ammonia water to adjust the pH of the solution to 11, stir at 50rpm for 10min, add 0.1mol / L hydrochloric acid dropwise to adjust the pH o...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com