Hemiplegia rehabilitation physiotherapy device for neurosurgery
A technology of neurosurgery and hemiplegia, applied in the field of medical equipment, can solve the problems of unsuitable and inconvenient use for patients with hemiplegia
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0053] refer to figure 1 and figure 2 , a neurosurgery hemiplegia rehabilitation physiotherapy device, mainly includes the following parts:
[0054] Support frame 1, as the main body support;
[0055] A reclining board 11 for lying down, on which an angle-adjustable backrest board 12 is installed;
[0056] Leg Lifting Assembly 2 for raising the patient's thigh;
[0057] A leg immobilization assembly 3 for immobilizing the patient's thigh;
[0058] A traction assembly 4 for traction of the patient's calf;
[0059] A traction adjustment assembly 5 for driving the traction assembly 4 to adjust the horizontal position and the vertical position;
[0060] And the arm exercising assembly 6 that is arranged on support frame 1 side.
[0061] refer to figure 1 and figure 2 , when the neurosurgical hemiplegia rehabilitation physiotherapy device is in use, the patient can lie on the lying board 11 on the support frame 1, and keep a half-lying state with his back on the backrest ...
Embodiment 2
[0074] The difference from Example 1 is that the surface of the couch 11 is coated with an antifouling coating. Since the couch 11 is used for patients to lie down, it will inevitably become dirty after a long time. For the convenience of cleaning the couch 11 , so a layer of antifouling coating is coated on the surface of the lying board 11, so a preparation method of the antifouling coating is provided, which has the advantages of short preparation process and simple preparation, wherein the antifouling coating on the surface of the lying board 11 The layers are prepared as follows:
[0075] Take the following ingredients by weight: 70 parts of chlorinated rubber, 30 parts of butyl acetate, 20 parts of ethyl acetate, 30 parts of butanol, 20 parts of cyclohexanone, 10 parts of dioctyl phthalate, tricresyl phosphate 10 parts, 10 parts of chlorinated paraffin, 20 parts of xylene, 10 parts of potassium oleate;
[0076] S1. Preparation of anti-fouling coating pre-preparation sol...
Embodiment 3
[0081] The difference from Example 2 lies in the preparation of the antifouling coating on the surface of the recliner 11, wherein the preparation method of the antifouling coating is as follows:
[0082] Take the following ingredients by weight: 72 parts of chlorinated rubber, 33 parts of butyl acetate, 20 parts of ethyl acetate, 30 parts of butanol, 23 parts of cyclohexanone, 10 parts of dioctyl phthalate, tricresyl phosphate 10 parts, 10 parts of chlorinated paraffin, 20 parts of xylene, 13 parts of potassium oleate;
[0083] S1. Preparation of anti-fouling coating pre-preparation solution: add chlorinated rubber, butyl acetate, ethyl acetate, butanol, and cyclohexanone to a mixer at 202°C for 30 minutes;
[0084] S2. Preparation of antifouling coating solution: add dioctyl phthalate, tricresyl phosphate, chlorinated paraffin, xylene, potassium oleate to the antifouling coating pre-preparation solution and stir evenly. After heat preservation treatment for 30 minutes It is...
PUM
![No PUM](https://static-eureka.patsnap.com/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka.patsnap.com/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com