Embodiment 1
[0029] see figure 1 , the preparation method of water-based ecological leather provided by the invention, it may further comprise the steps:
[0030] S1. Prepare the base cloth, pretreat the base cloth with the treatment liquid, and dry and iron the pretreated base cloth;
[0031] S2. Take the following raw materials by weight to prepare water-based polyurethane synthetic leather foam slurry: 70 parts of water-based polyurethane, 0.2 parts of dispersant, 2 parts of foam stabilizer, 0.2 parts of leveling agent, 2 parts of wetting agent, and 3 parts of thickener , 8 parts of mica powder, 10 parts of polypropylene powder and 6 parts of water-based color paste, water-based polyurethane, dispersant, leveling agent, wetting agent, thickener, mica powder, polypropylene powder and water-based color paste The raw materials are pre-mixed in the stirring tank, and after the stirring is completed, the pre-mixed slurry is bubbled by a bubble generator, and the water-based polyurethane syn...
Embodiment 2
[0044] see figure 1 , the preparation method of the water-based ecological leather provided by the invention comprises the following steps:
[0045] S1. Prepare the base cloth, pretreat the base cloth with the treatment liquid, and dry and iron the pretreated base cloth;
[0046] S2. Take the following raw materials by weight to prepare water-based polyurethane synthetic leather foaming slurry: 80 parts of water-based polyurethane, 0.3 parts of dispersant, 3 parts of foam stabilizer, 0.4 parts of leveling agent, 1.2 parts of wetting agent, and 2 parts of thickener , 7 parts of mica powder, 9 parts of polypropylene powder and 5 parts of water-based color paste, water-based polyurethane, dispersant, leveling agent, wetting agent, thickener, mica powder, polypropylene powder and water-based color paste The raw materials are pre-mixed in the stirring tank, and after the stirring is completed, the pre-mixed slurry is bubbled by a bubble generator, and the water-based polyurethane ...
Embodiment 3
[0058] see figure 1 , the preparation method of water-based ecological leather provided by the invention comprises the following steps:
[0059] S1. Prepare the base cloth, pretreat the base cloth with the treatment liquid, and dry and iron the pretreated base cloth;
[0060] S2. Take the following raw materials by weight to prepare water-based polyurethane synthetic leather foaming slurry: 80 parts of water-based polyurethane, 0.5 parts of dispersant, 4 parts of foam stabilizer, 0.4 parts of leveling agent, 1.5 parts of wetting agent, and 1.5 parts of thickener , 7 parts of mica powder, 8 parts of polypropylene powder and 5 parts of water-based color paste, water-based polyurethane, dispersant, leveling agent, wetting agent, thickener, mica powder, polypropylene powder and water-based color paste The raw materials are pre-mixed in the stirring tank, and after the stirring is completed, the pre-mixed slurry is bubbled by a bubble generator, and the water-based polyurethane sy...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 