A kind of gear oil with super long oil change period and preparation method thereof
A technology of oil change cycle and gear oil, which is applied in the field of lubricating oil, can solve problems such as short service life, and achieve good oxidation resistance, good compatibility, good sealing performance, clean dispersion and hydrophobicity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0047] This application document also discloses a method for preparing gear oil with super-long oil change intervals by using the above-mentioned raw materials, including the following steps:
[0048] Preparation of mixture A: Add olefinic synthetic oils PAO M300, PAO M100, PAO M30 and PAO M6, stir at 60-75°C for 25-35min, add pentaerythritol ester, stir at 60-75°C for 25-35min, mix, Then add polymethacrylate pour point depressant, stir at 60-75°C for 25-35 minutes, mix, dissolve the pour point depressant in synthetic oil, add viscosity index improver, stir at 60-75°C for 30 minutes -45min, mixed to obtain mixture A;
[0049] Preparation of mixture B: adding antirust agent, oily agent, detergent, extreme pressure antiwear agent and metal deactivator to alkylnaphthalene, stirring at constant temperature at 65-75°C for 25-35min, and mixing to obtain mixture B;
[0050] Preparation of mixture C: Mix mixture B and long-acting compounding agent, stir at 65-75°C for 25-35 minutes a...
preparation example 1
[0054] The preparation method of the long-acting composite agent comprises the following steps: in parts by weight: adding 0.4 parts of alkyl phosphate, 0.8 parts of octylamine and 0.8 parts of borate, stirring, raising the temperature to 120°C, and then stirring at constant temperature for 20 minutes;
[0055] Add 0.6 parts of sulfur-phosphorus organic molybdenum, stir, adjust the temperature to 65° C., and then stir at constant temperature for 30 minutes, wherein the sulfur-phosphorus organic molybdenum is selected from dialkyl molybdenum dithiophosphate.
preparation example 2
[0057] The preparation method of the long-acting composite agent comprises the following steps: in parts by weight: adding 0.3 parts of alkyl phosphate, 0.5 parts of octylamine and 0.5 parts of borate, stirring, raising the temperature to 110°C, and then stirring at constant temperature for 25 minutes;
[0058] Add 0.5 parts of sulfur-phosphorus organic molybdenum, stir, adjust the temperature to 60° C., and then stir at constant temperature for 35 minutes. The sulfur-phosphorus organic molybdenum is selected from nitrogen-containing dialkyl dithiophosphate oxymolybdenum.