Production method of high-upright-degree flat velvet cloth
A production method and flat technology, applied in the field of textile dyeing and finishing, can solve the problems of poor softness of flannelette, easy to produce wrinkled flannelette, fluff and looping, etc., and achieve the problem of poor softness, high standing, and increased density Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0048] Embodiment 1: flat silk polyester fleece
[0049] A method for producing flat velvet cloth with high uprightness, comprising the steps of:
[0050] 1. Gray fabric weaving: use 200D / 48F flat polyester filament (200D / 48F flat polyester filament has a monofilament thickness of 4.2D, wool height: 2.0±0.1mm, thickness 2.2-2.3mm), pile density (weft density) Achieve 210 roots / cm 2 , adopt W-type consolidation and V-type consolidation alternate pile spinning, and the ground weave adopts plain weave, the bristling roller adopts needle-type bristling roller, the diameter of the needle is 0.03mm, and the density of the needle is 3 pieces / cm 2 .
[0051] 2. Gray cloth brushing: After the gray cloth goes through the brushing process, the suede and disordered hairs are neatly combed. First put the cloth along the wool, brush the hair once, then put the cloth on the reverse wool, and brush the hair once; the speed is 9 m / min, the distance along the wool: 0.8mm, and the distance be...
Embodiment 2
[0068] Embodiment 2 flat silk polyester fleece
[0069] A method for producing flat velvet cloth with high uprightness, comprising the steps of:
[0070] 1. Gray fabric weaving: use 200D / 48F flat polyester filament (200D / 48F flat polyester filament has a monofilament thickness of 4.2D, wool height: 2.0±0.1mm, thickness 2.2-2.3mm), pile density (weft density) Achieve 210 roots / cm 2 , adopt W-type consolidation and V-type consolidation alternate pile spinning, and the ground weave adopts plain weave, the bristling roller adopts needle-type bristling roller, the diameter of the needle is 0.03mm, and the density of the needle is 3 pieces / cm 2 .
[0071] 2. Gray cloth brushing: After the gray cloth goes through the brushing process, the suede and disordered hairs are neatly combed. First put the cloth along the wool, brush the hair once, then put the cloth on the reverse wool, and brush the hair once; the speed is 9 m / min, the distance along the wool: 0.8mm, and the distance bet...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com