Problems solved by technology
Method used
Examples
Embodiment 1
[0023] An anti-cracking method suitable for a prefabricated inner partition wall, comprising the following steps:
[0024] S1: Select the materials required for the preparation of the inner partition wall, including lightweight partition boards, concrete, thermal insulation mortar, polyester fiber sound-absorbing materials, damping composite sound-absorbing materials, TPV-coated materials and assembled steel frames, and classify the materials ,spare;
[0025] S2: Prepare the anti-cracking outer film for the inner partition wall. The anti-cracking outer film for the inner partition wall includes epoxy cement material, silicone waterproof material, PVC film material, fireproof and antistatic material, epoxy resin grouting material, cement repair material, With cement repair materials as the main body, epoxy cement materials, silicone waterproof materials, PVC film materials, fireproof and antistatic materials, and epoxy resin grouting materials are mixed and used;
[0026] S3: ...
Embodiment 3
[0035] On the basis of Embodiment 1, a cracking prevention method suitable for a prefabricated interior partition wall includes the following steps:
[0036] S1: Select the materials required for the preparation of the inner partition wall, including lightweight partition boards, concrete, thermal insulation mortar, polyester fiber sound-absorbing materials, damping composite sound-absorbing materials, TPV-coated materials and assembled steel frames, and classify the materials ,spare;
[0037]S2: Prepare the anti-cracking outer film for the inner partition wall. The anti-cracking outer film for the inner partition wall includes epoxy cement material, silicone waterproof material, PVC film material, fireproof and antistatic material, epoxy resin grouting material, cement repair material, With cement repair materials as the main body, epoxy cement materials, silicone waterproof materials, PVC film materials, fireproof and antistatic materials, and epoxy resin grouting materials ...
Embodiment 4
[0059] On the basis of Embodiment 1, Embodiment 2 and Embodiment 3, an anti-cracking method suitable for a prefabricated interior partition wall includes the following steps:
[0060] S1: Select the materials required for the preparation of the inner partition wall, including lightweight partition boards, concrete, thermal insulation mortar, polyester fiber sound-absorbing materials, damping composite sound-absorbing materials, TPV-coated materials and assembled steel frames, and classify the materials ,spare;
[0061] S2: Prepare the anti-cracking outer film for the inner partition wall. The anti-cracking outer film for the inner partition wall includes epoxy cement material, silicone waterproof material, PVC film material, fireproof and antistatic material, epoxy resin grouting material, cement repair material, With cement repair materials as the main body, epoxy cement materials, silicone waterproof materials, PVC film materials, fireproof and antistatic materials, and epox...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com