Portland cement clinker
A Portland cement and clinker technology, applied in cement production and other directions, can solve problems such as not conducive to reducing production costs, not conducive to the protection of land resources, agricultural ecological environment and human living environment, etc. Natural environment, the effect of saving raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Portland cement clinker of the present invention, its raw material is by weight percentage by limestone, iron ore tailing sand, fly ash, pot bottom slag and pure iron fine powder and / or bauxite: limestone 74.5% (at 73 ~86% is feasible), iron ore tailings 10% (all are feasible within 5~18%), fly ash 12% (all are feasible within 2~12%), Bottom slag 3% (feasible in the range of 1-8%), pure iron fine powder and / or bauxite 0.5% (feasible in the range of 0-0.5%) for batching, according to conventional cement The production process processes it into cement clinker. Wherein the weight percent of pure iron fine powder and bauxite is: pure iron fine powder 70% (all feasible in the scope of 0~100%), 30% of bauxite (all feasible in the scope of 0~100%) of).
Embodiment 2
[0019] Portland cement clinker of the present invention, its raw material is by weight percent by limestone, iron ore tailing sand, fly ash, pot bottom slag and pure iron fine powder and / or bauxite: limestone 76.5% (at 76 ~83% is feasible), iron ore tailings 13% (all are feasible within 6~16%), fly ash 5% (all are feasible within 4~10%), Bottom slag 5% (feasible in the range of 1-5%), pure iron fine powder and / or bauxite 0.5% (feasible in the range of 0-0.5%) for batching, according to conventional cement The production process processes it into cement clinker. Wherein the weight percent of pure iron fine powder and bauxite is: pure iron fine powder 50% (all feasible in the scope of 0~100%), bauxite 50% (all feasible in the scope of 0~100%) of).
Embodiment 3
[0021] Portland cement clinker of the present invention, its raw material is by weight percentage by limestone, iron ore tailing sand, fly ash, pot bottom slag and pure iron fine powder and / or bauxite: limestone 80% (at 79 ~81% are feasible), iron ore tailings 11% (9~13% are feasible), fly ash 6% (6~8% are feasible), Bottom slag 2.7% (feasible in the range of 2-3%), pure iron fine powder and / or bauxite 0.3% (feasible in the range of 0-0.5%) for batching, according to conventional cement The production process processes it into cement clinker. Wherein the weight percent of pure iron fine powder and bauxite is: pure iron fine powder 30% (all feasible in the scope of 0~100%), 70% of bauxite (all feasible in the scope of 0~100%) of).
[0022] The Portland cement clinker of the present invention can utilize industrial waste slag and waste materials, and after batching, go through raw meal mill→raw meal bin→preheater→rotary kiln, and calcinate into Portland cement clinker at a hig...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com