Prepared agent of base course suitable to highway for intensifying waterproof performance of basal layer of roadbed
A technology for expressways and grassroots, applied in the field of waterproof enhancers, can solve the problems of shortening the service life of expressways, increasing maintenance funds and costs, and large maintenance times and workload, achieving good toughness, simple operation, and excellent water resistance and dispersion. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] The base compound is suitable for the waterproof reinforcement of expressway subgrade base, which is characterized in that it is prepared from the following raw materials according to the weight ratio: water: 5.01 sodium silanolate: 1.188 sodium silicate: 2.97 pure acrylic emulsion: 0.505;
[0019] The production process of the present invention is as follows: according to the above weight ratio, sodium siliconate, sodium silicate and water are mixed and stirred for 40 minutes, then pure acrylic emulsion is added and stirred for 40 minutes to obtain the finished product.
Embodiment 2
[0021] Choose according to 1000 grams of raw material total amount of the present invention, wherein, choose raw material water 515.5 grams, sodium silanolate 123.7 grams, sodium silicate 309.3 grams, pure acrylic emulsion 51.5 grams. Sodium silanolate, sodium silicate and water were mixed and stirred for 30 minutes according to the above weight, then pure acrylic emulsion was added and stirred for 60 minutes to obtain the finished product.
[0022] The finished product of the present invention belongs to silicone-modified acrylic acid water-based environment-friendly formulation, one-component, white emulsion in appearance, and its temperature resistance range: before reaction: -15℃~+18℃, after reaction: -45℃~+ 160℃; PH value: 13.0±0.5; viscosity: 7.0~9.0mpa.s; free formaldehyde content≤0.1g / kg; VOC content≤200g / L; W(Pb) content≤90mg / kg; W(Hg) content ≤60mg / kg.
Embodiment 3
[0024] The using method of finished product of the present invention is as follows:
[0025] 1. Roll the base layer into shape.
[0026] 2. Spray a sufficient amount of this solution evenly on the surface of the base layer by spraying.
[0027] 3. Spray once if the penetration thickness is not enough, you can spray the second time, but it must be done before the first time is dry.