Embodiment 1
[0015] Example 1: 65.20 kg of water was poured into the stirring tank, and 6.0 kg of polyvinyl alcohol, 0.5 kg of fluorescent whitening agent, 16 kg of titanium dioxide, 10 kg of gray calcium, 1.0 kg of urea, and tributyl phosphate were sequentially added during the stirring process. 1.0 kg, 0.3 kg of 1,2-benzisothiazolin-3-one, heated to 60-70°C under normal pressure and then kept stirring for no less than 0.5-1 hour. After all the materials were dissolved, stop the heat preservation. When the above mixture is evenly stirred until it becomes transparent and no agglomeration powder, filter it with a 80-mesh filter sieve at a medium speed, and then store it in barrels after cooling. Manufactured products of tempered paint.
[0016] For the dosage of various materials in Examples 2 to 6, please refer to Table 1, which will not be described in detail; for other content such as production steps, please refer to Example 1, and will not be described in detail.
[0017] Table 1: Com...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com