Embodiment 1
[0034] Example 1: Bio-gel seed coating agent includes 50 grams of polypropylene milling ammonium, 100 grams of sodium carboxymethyl starch, 2000 grams of calcium bentonite, 3000 grams of talc, 200 grams of artemisia seed gum, and 100 grams of carboxymethyl cellulose .
[0035] The preparation method includes the following steps: the preparation process is carried out at room temperature,
[0036] (1) According to the proportion of polypropylene milled ammonium, sodium carboxymethyl starch, artemisia seed gum and carboxymethyl cellulose with ultra-fine grinding equipment, pulverize, filter and mix for more than 30 minutes, and inspect the fineness of the powder, which is required to reach 500 Above
[0037] (2) Crush, filter and mix talc powder and calcium-based bentonite according to the ratio with ultra-fine grinding equipment for more than 30 minutes, and inspect the fineness of the powder, which requires more than 500 mesh;
[0038] (3) Mix the two mixtures obtained in steps (1...
Embodiment 2
[0040] Example 2: Bio-gel seed coating agent includes 500 grams of polyacrylate, 600 grams of sodium carboxymethyl cellulose, 5000 grams of sodium bentonite, 7000 grams of talc, 1500 grams of artemisia seed gum, and 1000 grams of carboxymethyl cellulose , 800 grams of zeolite powder.
[0041] The preparation method includes the following steps: the preparation process is carried out at room temperature,
[0042] (1) According to the proportion of polyacrylate, sodium carboxymethyl cellulose, artemisia seed gum, carboxymethyl cellulose and zeolite powder, pulverize, filter and mix for more than 30 minutes with ultra-fine grinding equipment to check the fineness of the powder. It is required to reach more than 500 meshes;
[0043] (2) Crush, filter and mix talc powder and calcium-based bentonite according to the ratio with ultra-fine grinding equipment for more than 30 minutes, and inspect the fineness of the powder, which requires more than 500 mesh;
[0044] (3) Mix the two mixtur...
Embodiment 3
[0046] Example 3: Bio-gel seed coating agent includes 250 grams of polyvinyl alcohol, 350 grams of sodium carboxymethyl cellulose and sodium carboxymethyl starch, 3500 grams of sodium bentonite and calcium bentonite, 5000 grams of talcum powder, and artemisia seed gum 850 grams, 550 grams of carboxymethyl cellulose, 450 grams of zeolite powder.
[0047] The preparation method includes the following steps: the preparation process is carried out at room temperature,
[0048] (1) Crush, filter and mix polyvinyl alcohol, sodium carboxymethyl cellulose, sodium carboxymethyl starch, artemisia seed gum, carboxymethyl cellulose and zeolite powder in an ultrafine grinding equipment for more than 30 minutes in proportion , To check the fineness of the powder, it is required to reach 500 meshes or more;
[0049] (2) Crush, filter and mix talc powder, calcium-based bentonite and sodium-based bentonite in proportions with ultrafine grinding equipment for more than 30 minutes, and inspect the f...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com