A technology of rapeseed oil and fatliquor, which is applied in animal husbandry, chemical treatment and application of small raw hide/big raw hide/leather skin/fur, and can solve the problem that it is easy to be extracted by water or organic solvent and is not suitable for the production of waterproof leather , Insufficient leather fatliquoring effect, etc., to achieve the effect of increasing fullness, significant filling effect, and easy operation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0044] Add 100g of rapeseed oil and 15g of maleic anhydride to a three-necked flask equipped with a magnetic stirrer, heat up to 60°C, stir the two evenly, add 2.3g of initiator azodiethylbutyronitrile, heat up to about 125°C, Constant temperature for 1 hour, add 3.5g styrene, continue constant temperature for 3 hours, cool to normal temperature, add dropwise 3g of 98% concentrated sulfuric acid, stir for 15 minutes, let stand for 2 hours, neutralize with sodium hydroxide to a pH value of 7.
Embodiment 2
[0046] Add 100g of rapeseed oil and 18g of maleic anhydride to a three-necked flask equipped with a magnetic stirrer, raise the temperature to 70°C, stir the two evenly, add 3.0g of initiator benzoyl peroxide, raise the temperature to about 95°C, and keep the temperature constant 0.5 hours, add 4.5g of vinyl acetate, continue to keep constant temperature for 3 hours, cool to room temperature, add 2.5g of 98% concentrated sulfuric acid dropwise, stir for 15 minutes, let stand for 2 hours, neutralize with 30% NaOH aqueous solution until the pH value is 7 .
Embodiment 3
[0048] Add 100g of rapeseed oil and 10g of maleic anhydride to a three-necked flask equipped with a magnetic stirrer, heat up to 80°C, stir the two evenly, add 2.0g of initiator azodiethylbutyronitrile, heat up to about 125°C, Constant temperature for 1 hour, add 1.5g styrene, continue constant temperature for 3 hours, cool to normal temperature, add dropwise 5g of 98% concentrated sulfuric acid, stir for 15 minutes, let stand for 2 hours, neutralize with 30% NaOH aqueous solution until the pH value is 7.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com