Production method of non-woven woolen lining cloth
A production method and non-woven technology, applied in the direction of non-woven fabrics, textiles and papermaking, etc., can solve problems such as difficulty in achieving performance, harmony and unity, and performance differences, and achieve full hand feeling, uniform cloth surface, elasticity and dimensional stability Good results
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Production of wool fiber and polyester fiber mixed fiber nonwoven interlining with PA (polyester) and PES (polyamide) coating, the weight ratio of wool fiber and polyester fiber is 80:20, and the mass per unit area of the base fabric is 60g / m 2 , coating size is 20g / m 2 .
[0016] The production method of this non-woven wool interlining comprises the steps:
[0017] ①In the spunlace nonwoven production line, carbonized wool fiber (length about 20 μm) and polyester fiber (fineness 1.2dtex, length 38mm) are fed into the cotton feeding machine at a weight ratio of 80:20, through opening and impurity removal , mixed, and carded into a fiber web, the speed of the production line is 45m / min,
[0018] ②Put the fiber mesh in step ① through the hydroentanglement machine for hydroentanglement reinforcement;
[0019] ③ Dry and wind the product obtained in step ② to make the required base fabric for the production of interlining, and control the weight per unit area at 60g / m...
Embodiment 2
[0023] Production of mixed fiber nonwovens of carbonized wool fiber and nylon fiber with PA coating, the weight ratio of wool fiber and nylon fiber is 40:60, and the unit area of the base fabric is 30g / m 2 , the amount of sizing is 12g / m 2 .
[0024] The production method of this non-woven wool interlining comprises the steps:
[0025] ①In the hot-rolled nonwoven production line, nylon fiber (fineness 1.5dtex, length 45mm) and wool fiber (length about 18μm) are fed into the cotton feeding machine at a weight ratio of 60:40, through opening, impurity removal, Mixing, finally combing into fiber web, the production line speed is 30m / min;
[0026] ②The fiber web in step ① is thermally bonded and reinforced through a hot rolling mill;
[0027] ③ Wind the product obtained in step ② to make the required base fabric for the production of interlining, and control the grammage at 30g / m 2 ;
[0028] ④In the interlining production line, the base fabric is fed into the base fabric f...
PUM
| Property | Measurement | Unit |
|---|---|---|
| length | aaaaa | aaaaa |
| length | aaaaa | aaaaa |
| particle diameter | aaaaa | aaaaa |