Method for preparing polyferose
A technology of polysaccharide iron and water iron, which is applied in the field of polysaccharide iron production and can solve the problems of methanol toxicity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] At room temperature, 360 grams of ferric chloride hexahydrate and 750 grams of water were added into the reactor to dissolve into an aqueous solution of ferric chloride. Adding reduction value DE is 780 grams of oligosaccharide syrup of 71%, and the solid sugar content of oligosaccharide syrup is 26.5%. Stir, and continuously and uniformly add a sodium carbonate aqueous solution with a concentration of 0.2 (W / W) until Fe(OH) is generated 3 Precipitation, the solution is still acidic at this time. The feeding time of the aqueous sodium bicarbonate solution was 35 minutes. After stirring for 15 minutes, within 20 minutes, a sodium hydroxide aqueous solution with a concentration of 0.3 (W / W) was continuously and uniformly added until the pH value of the solution was 11.6. The temperature of the reaction kettle was raised to make the temperature of the reaction solution reach 81° C., and after keeping for 20 minutes, the reaction solution was cooled to room temperature. ...
Embodiment 2
[0017] At 10°C, add 18 kg of ferric chloride hexahydrate and 45 kg of water into the reaction kettle to dissolve into an aqueous solution of ferric chloride. Adding reduction value DE is 39 kilograms of oligosaccharide syrup of 69%, and the solid sugar content of oligosaccharide syrup is 26.1%. Stir, and continuously and uniformly add a sodium carbonate aqueous solution with a concentration of 0.3 (W / W) until Fe(OH) is generated 3 Precipitation, the solution is still acidic at this time. The feeding time of the aqueous sodium bicarbonate solution was 45 minutes. After stirring for 20 minutes, within 25 minutes, a sodium hydroxide aqueous solution with a concentration of 0.3 (W / W) was continuously and uniformly added until the pH value of the solution was 11.6. The temperature of the reaction kettle was raised to make the temperature of the reaction solution reach 78° C., and after keeping for 20 minutes, the reaction solution was cooled to room temperature. The reaction sol...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com