A formaldehyde elimination agent and formaldehyde technology, applied in the direction of separation methods, chemical instruments and methods, aldehyde/ketone condensation polymer adhesives, etc., can solve the problem of low formaldehyde release, achieve cost reduction, low production cost, and easy operation convenient effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0033] 1. Prepare raw materials according to the following weight ratio:
[0034] Formaldehyde (concentration 37%): 200kg
[0035] Water: 300kg
[0037] Borax: 1kg
[0038] Urea: 350kg
[0039] Sodium hydroxide solution (30% concentration): 2kg
[0040] 2. Add the above raw materials into the reaction kettle in turn, start stirring when adding, control the heating temperature at 40°C, and stir well;
[0041] 3. Stir until it is completely dissolved, take a sample to observe the solution, if there is no suspended matter, check the pH value, and finally adjust the pH value to 8.5-9.0 with a 30% sodium hydroxide solution, continue to stir until it is in a stable state, take a sample for analysis, and store it for later use .
[0042] The technical indicators of the product are shown in Table 1.
[0043] solid content
[0044] Although the heating temperature in this embodiment is 40°C, it can be controlled at any temperature value ...
Embodiment 2
[0046] 1. Prepare raw materials according to the following weight ratio:
[0047] Formaldehyde (concentration 37%): 200kg
[0048] Water: 200kg
[0050] Borax: 1kg
[0051] Urea: 350kg
[0052] Ammonia water (concentration 25%): 12kg
[0053] 2. Except that the heating temperature is 20° C. and the pH value is 7.5-8.0, other steps are the same as in Example 1.
[0054] The technical indicators of the product are shown in Table 2.
[0055] solid content
Embodiment 3
[0057] 1. Prepare raw materials according to the following weight ratio:
[0058] Formaldehyde (concentration 37%): 200kg
[0059] Water: 300kg
[0061] Borax: 0.1kg
[0062] Urea: 400kg
[0063] Ammonia water (concentration 25%): 15kg
[0064] 2. Except that the heating temperature is 50° C. and the pH value is 7.5-8.0, other steps are the same as in Example 1.
[0065] The technical indicators of product technical indicators are shown in Table 3
[0066] solid content
PUM
Property | Measurement | Unit |
---|---|---|
strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com