[0009] 60% high alumina powder, 10% talc powder, 3% silica powder, 3% bentonite, 11% fluorite powder are used as raw materials, 8% borax and 2% sodium tripolyphosphate are used as binders. 3% tartaric acid is used as a preservative, and these components are all added to a mixer and stirred evenly, then an appropriate amount of water is added, and mixed and stirred to form a paste coating. After the castable material on the inner wall of the garbage incinerator is poured and demoulded, the paint is manually applied to the castable material on the inner wall of the garbage incinerator, and the sintering is completed at high temperature. After sintering, the service life of the inner wall of the entire garbage incinerator can reach 10 months.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com