[0017] The preparation method of 2-propynyl 2-hydroxyalkyl ether is to add 1 mol of propynyl alcohol and 0.01 mol of sodium hydroxide to a 1000ml pressure-resistant reaction flask, heat it to 50°C in a water bath, and stir to dissolve it completely , then at a pressure of 0.1 MPa N 2 Under the protection, add 1mol of propylene oxide and react at 50°C for 1 hour, then add 1mol of ethylene oxide, react at 70°C for 1.5 hours, and finally control the temperature at 50°C and keep the temperature for 1 hour to obtain the product of the present invention. 2-Propynyl-2-hydroxyalkyl ether. The 2-propynyl-2-hydroxyalkyl ether can be used as nickel plating intermediate in nickel leveling agent and brightener.
Embodiment 2
[0019] The preparation method of 2-propynyl-2-hydroxyalkyl ether, which is to add 5mol of propynyl alcohol and 0.01mol of sodium hydroxide to a 1000ml pressure-resistant reaction flask, heat to 90°C in a water bath, and stir to make it thoroughly melted, then at a pressure of 0.6 MPa N 2 Under protection, add 1 mol of propylene oxide, react at 60 ° C for 1.5 hours, then add 1 mol of ethylene oxide, react at 80 ° C for 1 hour, and finally control the temperature at 90 ° C and keep the temperature for 5 hours to obtain the method described in the present invention. Product 2-propynyl-2-hydroxyalkyl ether. The 2-propynyl-2-hydroxyalkyl ether can be used as nickel plating intermediate in nickel leveling agent and brightener.
Embodiment 3
[0021] The preparation method of 2-propynyl-2-hydroxyalkyl ether is to add 1 mol of propynyl alcohol and 0.03 mol of sodium hydroxide to a 1000ml pressure-resistant reaction flask, heat it to 70°C in a water bath, and stir to make it thoroughly melted, then at a pressure of 0.3 MPa N 2 Under protection, add 5mol of propylene oxide and react at 55°C for 1.2 hours, then add 5mol of ethylene oxide, react at 75°C for 1.3 hours, and control the temperature at 70°C for 3 hours to obtain the product of the present invention. 2-Propynyl-2-hydroxyalkyl ether. The 2-propynyl-2-hydroxyalkyl ether can be used as nickel plating intermediate in nickel leveling agent and brightener.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com