Sealing corrosion proof protection method of rope-suspension bridge cable system
An anti-corrosion and suspension bridge technology, which can be used in devices, coatings, and metal material coating processes for coating liquids on surfaces. Insufficient corrosion age, etc., to achieve stable and excellent adhesion and paintability, good recoating and repair performance, and excellent weather resistance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0057] 1. Perform the following treatments on the outer surface of the main cable of the wrapped wire section in sequence:
[0058] First remove the dirt on the surface of the galvanized steel wire of the main cable and perform drying treatment; then apply one layer of nano-modified epoxy sealing paint on the outer surface of the main cable steel wire with a thickness of 20-40 μm; wait for the sealing paint to dry naturally for 24 hours and paint After the film is dry, apply silane-modified polyether sealant to fill the gap between the steel wires of the main cable and shape it into a basic smooth curve; then use a wire winding machine to wind a layer of galvanized steel wires with a diameter of 4.0mm in close rows; remove the surface of the wound steel wires Dirt and excess sealant squeezed out; then coat one layer of nano-modified epoxy sealant on the surface of the main cable winding steel wire, with a thickness of 20-40μm; then coat with silane-modified polyether sealant an...
Embodiment 2
[0072] 1. Perform the following treatments on the outer surface of the main cable of the wrapped wire section in sequence:
[0073] First remove the dirt on the surface of the galvanized steel wire of the main cable and perform drying treatment; then apply a layer of nano-modified epoxy sealing paint on the outer surface of the main cable steel wire with a thickness of 30 μm; wait for the sealing paint to dry naturally for 24 hours and the paint film is hard Finally, apply silane-modified polyether sealant, fill the gap between the steel wires of the main cable and shape it into a basic smooth curve; then use a wire winding machine to wind a layer of galvanized steel wires with a diameter of 4.0mm; remove the dirt on the surface of the wound steel wires and the excess sealant extruded; then coat one layer of nano-modified epoxy sealant on the surface of the main cable winding steel wire with a thickness of 30 μm; then apply silane-modified polyether sealant to fill the gap betw...
Embodiment 3
[0086] Embodiment 3: (E.1) Before being installed on the bridge, carry out arc spraying anodic metal coating anticorrosion treatment to cable clip, loose cable saddle (cover) and saddle;
[0087] Said arc spraying anodic metal coating, the metal wire used for arc spraying in the coating is aluminum wire, and the aluminum content in the aluminum wire is greater than or equal to 99.5%. The diameters of the two metal wires used in arc spraying are equal to 3 mm; the thickness of the sprayed metal coating is 300 μm.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
tensile strength | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com