Method for separating molybdenum and bismuth sulfide minerals
A separation method and mineral technology, applied in the direction of solid separation, flotation, etc., can solve problems such as inconvenient operation, achieve the effects of improving production conditions, less consumption, and reducing environmental pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] Mineral Type 1: The molybdenum-bismuth mixed concentrate is obtained after the raw ore undergoes molybdenum-bismuth mixed flotation, containing 7.54% molybdenum and 15.35% bismuth. The molybdenum-bismuth mixed concentrate is added in the order of water glass, new inhibitor, and kerosene respectively. And stirring, after one roughing, three times of beneficiation, and two sweepings, the molybdenum concentrate containing 46.12% molybdenum and 0.63% bismuth can be obtained. (The water glass consumption of adding is 620g / t, and the consumption of the new inhibitor of adding is 600g / t, and the kerosene consumption of adding is 120g / t.)
Embodiment 2
[0029] Mineral type 2, the molybdenum-bismuth mixed concentrate is obtained after the raw ore undergoes molybdenum-bismuth mixed flotation, containing 8.36% molybdenum and 12.55% bismuth. And stirring, after one roughing, three times of beneficiation, and two sweepings, the molybdenum concentrate containing 45.82% molybdenum and 0.53% bismuth can be obtained. (The water glass consumption of adding is 800g / t, and the consumption of the new inhibitor of adding is 650g / t, and the kerosene consumption of adding is 130g / t.)
Embodiment 3
[0031] Mineral Type 3: The molybdenum-bismuth mixed concentrate is obtained after molybdenum-bismuth mixed flotation, which contains 9.59% molybdenum and 15.05% bismuth. The molybdenum-bismuth mixed concentrate is added in the order of water glass, new inhibitor, and kerosene respectively. And stirring, after one roughing, three times of beneficiation, and two sweepings, the molybdenum concentrate containing 46.52% molybdenum and 0.68% bismuth can be obtained. (The water glass consumption of adding is 850g / t, and the consumption of the new inhibitor of adding is 700g / t, and the kerosene consumption of adding is 130g / t.)
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com